EMS-Grivory Grivory® XE 4185 black 9453 PA*

Category Polymer , Thermoplastic , Nylon
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® XE 4185 black 9453 PA*.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product description: Grivory XE 4185 is a non-reinforced heat stabilized engineering thermoplastic material based on a semicrystalline, partially aromatic copolyamide. ISO polymer designation: PA 10T/X ASTM designation: PPA, polyphthalamide The main distinguishing features of Grivory HT, when compared to other polyamides, are its good performance at high temperatures providing parts which are stiffer, stronger, have better heat distortion and dimensional stability as well as excellent chemical resistance and low moisture absorption. Grivory XE 4185 is especially suitable for injection molded components in electrical and electronic applications. The material is suitable for lead-free SMT reflow soldering e.g. JEDEC J-STD-020C (peak temperature 260°C). Components conforming to JEDEC MSL1 are achievable.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.18 g/cc
0.0426 lb/in³
ISO 1183
Water Absorption 3.9 %
3.9 %
ISO 62
Moisture Absorption 1.70 %
1.70 %
ISO 62
Linear Mold Shrinkage, Flow 0.020 cm/cm
0.020 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.020 cm/cm
0.020 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Ball Indentation Hardness 150 MPa
21800 psi
dry; ISO 2039-1
150 MPa
21800 psi
conditioned; ISO 2039-1
Tensile Strength at Break 60.0 MPa
8700 psi
dry; ISO 527-1/-2
60.0 MPa
8700 psi
conditioned; ISO 527-1/-2
Elongation at Break 6.5 %
6.5 %
dry; ISO 527-1/-2
12 %
12 %
conditioned; ISO 527-1/-2
Tensile Modulus 3.00 GPa
435 ksi
conditioned; ISO 527-1/-2
3.00 GPa
435 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 3.50 J/cm²
16.7 ft-lb/in²
conditioned; ISO 179/1eU
4.00 J/cm²
19.0 ft-lb/in²
dry; ISO 179/1eU
3.00 J/cm²

@Temperature 30.0 °C
14.3 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
3.50 J/cm²

@Temperature 30.0 °C
16.7 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
dry; ISO 179/1eA
0.500 J/cm²
2.38 ft-lb/in²
conditioned; ISO 179/1eA
0.300 J/cm²

@Temperature 30.0 °C
1.43 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
0.300 J/cm²

@Temperature 30.0 °C
1.43 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 80.0 µm/m-°C
44.4 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C
44.4 µin/in-°F
ISO 11359-1/-2
Melting Point 315 °C
599 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 140 °C
284 °F
long term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 185 °C
365 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
230 °F
ISO 75-1/-2
Flammability, UL94 V-0
V-0
IEC 60695-11-10
V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
dry; IEC 60093
1.00e+11 ohm-cm
1.00e+11 ohm-cm
conditioned; IEC 60093
Surface Resistance 1.00e+11 ohm
1.00e+11 ohm
IEC 60093
Dielectric Strength 30.0 kV/mm
762 kV/in
dry; IEC 60243-1
30.0 kV/mm
762 kV/in
conditioned; IEC 60243-1
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Air intake sytems
Automotive electr. and electronics, lighting
Compressed air systems
Fuel systems
Hydraulic systems
Interior
Electricals & Electronics Connectors
Electrical appliances
Electrical equipment
Energy distribution
Lighting
Mobile phones and other portable devices
Form Granules
Industry & Consumer goods Hydraulics & Pneumatics
Mechanical Engineering
Power transmission
Tools & Accessories
Processing Injection Molding
Product Attributes Bio based Polyamide
Co Polyamide
Hydrolysis resistant
Improved alcohol resistance
Improved flowability and demoulding
Partially aromatic Polyamide
Special Characteristics Flame retardant
Improved heat resistance