Material Notes:
Data was collected by ISO methods and provided by BASF.
Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
Linear Mold Shrinkage, Flow 0.013 cm/cm
0.013 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 22.0 MPa
3190 psi
Elongation at Break 20 %
20 %
Tensile Modulus 2.50 GPa
363 ksi
Charpy Impact Unnotched 3.50 J/cm²
16.7 ft-lb/in²
1.00 J/cm²

@Temperature -30.0 °C
4.76 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 55.0 µm/m-°C

@Temperature 20.0 °C
30.6 µin/in-°F

@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 125 °C
257 °F
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C
167 °F