Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polykemi AB SCANFILL BOTTLE BY45C2 Blow Molding Grade

Category Polymer , Thermoplastic
Manufacturer Polykemi AB
Trade Name SCANFILL
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polykemi AB SCANFILL BOTTLE BY45C2 Blow Molding Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Polykemi AB
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
ISO 1183
Filler Content 45 %
45 %
±2%; Polykemi
Melt Index of Compound 0.10 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.10 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break <= 20.0 MPa
<= 2900 psi
ISO/R527
Elongation at Yield 15 %
15 %
ISO/R527
Flexural Strength <= 31.0 MPa
<= 4500 psi
ISO 178
Flexural Modulus 1.80 GPa

@Temperature 23.0 °C
261 ksi

@Temperature 73.4 °F
ISO 178
Charpy Impact Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179
NB

@Temperature -20.0 °C
NB

@Temperature -4.00 °F
ISO 179
Charpy Impact, Notched 1.80 J/cm²

@Temperature -20.0 °C
8.57 ft-lb/in²

@Temperature -4.00 °F
ISO 179
2.80 J/cm²

@Temperature 23.0 °C
13.3 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C
185 °F
120°C/h; ISO 75/1
Deflection Temperature at 1.8 MPa (264 psi) 42.0 °C
108 °F
120°C/h; ISO 75/1
Vicat Softening Point 68.0 °C

@Load 5.001 kg
154 °F

@Load 11.03 lb
50°C/h; ISO 306
125 °C

@Load 1.00 kg
257 °F

@Load 2.21 lb
50°C/h; ISO 306
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved