Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Sax Polymers SAXLAC 310U Acrylonitrile Butadiene Styrene

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
Manufacturer Sax Polymers
Trade Name SAXLAC
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sax Polymers SAXLAC 310U Acrylonitrile Butadiene Styrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Saxalac 310U is an antistatic, high impact resistant and light stabilized ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% RH.Information provided by SAX Polymers
Physical Properties Metric English Comments
Density 1.02 g/cc
0.0368 lb/in³
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
Melt Flow 7.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
7.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
from MVR; ISO 1033
Mechanical Properties Metric English Comments
Tensile Strength 40.0 MPa
5800 psi
ISO 527-1
Elongation at Break 4.0 %
4.0 %
ISO 527-1
Tensile Modulus 1.90 GPa
276 ksi
ISO 527-1
Izod Impact, Notched (ISO) 15.0 kJ/m²

@Temperature -30.0 °C
7.14 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
30.0 kJ/m²

@Temperature 23.0 °C
14.3 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Izod Impact, Unnotched (ISO) 100 kJ/m²

@Temperature 23.0 °C
47.6 ft-lb/in²

@Temperature 73.4 °F
ISO 180
100 kJ/m²

@Temperature -30.0 °C
47.6 ft-lb/in²

@Temperature -22.0 °F
ISO 180
Charpy Impact Unnotched 10.0 J/cm²

@Temperature 23.0 °C
47.6 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
10.0 J/cm²

@Temperature -30.0 °C
47.6 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 1.40 J/cm²

@Temperature -30.0 °C
6.66 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
2.80 J/cm²

@Temperature 23.0 °C
13.3 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Hot Ball Pressure Test 95.0 °C

@Thickness 2.00 mm
203 °F

@Thickness 0.0787 in
IE/CEN 60335-1
Deflection Temperature at 1.8 MPa (264 psi) 92.0 °C
198 °F
80*10*4 s=60mm; ISO 75-1 a
Vicat Softening Point 96.0 °C
205 °F
50B; ISO 306
Flammability, UL94 HB
HB
Glow Wire Test 650 °C
1200 °F
IE/CEN 60695-2-12
Processing Properties Metric English Comments
Melt Temperature 220 - 260 °C
428 - 500 °F
Mold Temperature 60.0 - 90.0 °C
140 - 194 °F
Drying Temperature 80.0 °C

@Time 7200 - 14400 sec
176 °F

@Time 2.00 - 4.00 hour
Moisture Content <= 0.20 %
<= 0.20 %