Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ascend Performance Materials Vydyne® R515 Nylon 66, 15% Glass Reinforced, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 20% Glass Fiber Filled
Manufacturer Ascend Performance Materials (formerly Solutia)
Trade Name VYDYNE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ascend Performance Materials Vydyne® R515 Nylon 66, 15% Glass Reinforced, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Vydyne® R515 is general-purpose, 15% glass-fiber reinforced PA66 resin. Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 15% Filler by WeightAdditive:Lubricant Features: Gasoline ResistanceGood Chemical ResistanceGood FlowGood Mold ReleaseGrease ResistantHeat StabilizedHigh RigidityHigh StrengthLubricatedOil ResistantSolvent ResistantUses:Automotive Under the HoodGearsHousingsPower/Other ToolsAppearance: Natural ColorForms: PelletsProcessing Method: Injection MoldingInformation provided by Ascend Performance Materials.
Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
ISO 1183
Water Absorption 1.0 %

@Time 86400 sec
1.0 %

@Time 24.0 hour
ISO 62
Moisture Absorption at Equilibrium 2.2 %
2.2 %
50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0050 cm/cm

@Diameter 2.00 mm
0.0050 in/in

@Diameter 0.0787 in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.010 cm/cm

@Diameter 2.00 mm
0.010 in/in

@Diameter 0.0787 in
ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength, Yield 80.0 MPa
11600 psi
ISO 527-2
Elongation at Break 13 %
13 %
ISO 527-2
Tensile Modulus 4.00 GPa
580 ksi
ISO 527-2
Flexural Strength 110 MPa
16000 psi
ISO 178
Flexural Modulus 3.25 GPa
471 ksi
ISO 178
Izod Impact, Notched (ISO) 5.40 kJ/m²

@Temperature -30.0 °C
2.57 ft-lb/in²

@Temperature -22.0 °F
ISO 180
7.00 kJ/m²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Charpy Impact Unnotched 3.80 J/cm²

@Temperature -30.0 °C
18.1 ft-lb/in²

@Temperature -22.0 °F
ISO 179
4.30 J/cm²

@Temperature 23.0 °C
20.5 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Charpy Impact, Notched 0.530 J/cm²

@Temperature -30.0 °C
2.52 ft-lb/in²

@Temperature -22.0 °F
ISO 179
0.750 J/cm²

@Temperature 23.0 °C
3.57 ft-lb/in²

@Temperature 73.4 °F
ISO 179