Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.250 J/cm² @Temperature 23.0 °C |
1.19 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom PLASTAMID® 66 BT B 27 A PA66 PA66 for compounding, modified for general use, with excellent manufacturing properties. Use: automotive, engineering, electrical and consumer-goods industry - electrical tools, fasteners, clamps, h.. |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature 23.0 °C |
1.19 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 6 FRC 2 Polyamide 6, Halogen Free Flame Retardant FeaturesPA 6 for injection moulding with increased flammability resistance with non-halogen flame retardant. Determined for electro-technical purposes. Excellent flow of the material predetermines.. |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature 23.0 °C |
1.19 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVAMID 6 FRM 1 PA6, flame retardant FeaturesDetermined for electrotechnical use. Delivered in natural mode. PA 6 for injection moulding with reduced flammability, with nonhalogen flame retardant. Excellent fluidity of the material pre.. |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature 23.0 °C |
1.19 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVAMID 6 GF 20 PA6, 20% glass beads FeaturesNearly ideal anisotropy of shrinkage in the vertical and in the horizontal direction is established. Manufacturing of exact mouldings. Disadvantage are the relatively low mechanical properti.. |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature 23.0 °C |
1.19 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVASTER® B1 GF 15 FRX 5 PBT reinforced with 15% glass fibre, with flame retardant Features: PBT with the content of 15 % chemically bound glass fibre and with the halogen freeflame retardant. Anisotropy of shrinkage enables the injection moulding of round, cylindrical or other ho.. |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature -20.0 °C |
1.19 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PPH T2020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature -20.0 °C |
1.19 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PPH TS15020 D Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature -20.0 °C |
1.19 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PPH TS15020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature -20.0 °C |
1.19 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PPHC T15020 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature -20.0 °C |
1.19 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVALEN PC 99 GF 30/1M Polypropylene reinforced with glass fiber, improved flowing Modified copolymer PP for injection molding, reinforced with 30% glass fiber, improved flowing. Applied in all industry branches. Delivered in natural mode and in the full RAL color scale.Informatio.. |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature 23.0 °C |
1.19 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVAMID 6 FRC 2 218/1M PA6, flame retardant Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0.. |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature -20.0 °C |
1.19 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PPH T1040 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature -20.0 °C |
1.19 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PPH T2040 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature -20.0 °C |
1.19 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PPH T5020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature -30.0 °C |
1.19 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Inno-Comp INNOPOL® CS 2-4120 20% Talc-Filled Polypropylene Block-Copolymer INNOPOL® CS 2-4120 is a 20% talc-filled compound based on polypropylene block-copolymer. This grade is available in nature and custom colored form as well.INNOPOL® CS 2-4120 is developed for p.. |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature -20.0 °C |
1.19 ft-lb/in² @Temperature -4.00 °F |
|
LATI Latamid 68 H2-V0 PA6/PA66 copolymer, Heat Stabilized, Flame Retardant PA6/PA66 copolymer (PA6/PA66) based compound. Heat stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Good surface appearance.Availability: Africa & Middle Ea.. |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature 23.0 °C |
1.19 ft-lb/in² @Temperature 73.4 °F |
|
LATI Latan 13 K/30 POM, 30% Carbon Fiber Reinforced Polyoxymethylene (POM) based compound. Carbon fiber. Medium viscosity. Good tribological properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation .. |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature 23.0 °C |
1.19 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Solvay TECHNYL® A 221 Natural FA PA66, DRY Description: Product in development. Unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for fast cycles. Suitable for food contact applicationsAv.. |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature -20.0 °C |
1.19 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Borealis BH980MO Polypropylene Copolymer BH980MO is a heterophasic copolymer. This grade provides very high stiffness, high gloss and low stress whitening. and is designed for high-speed injection molding and contains nucleating and antist.. |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature -20.0 °C |
1.19 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Borealis Daplen™ EG250AI Polypropylene TPO Compound Daplen™ EG250AI is a 20% mineral reinforced impact modified polypropylene compound suitable for injection molding. This material has an excellent balance between impact strength and stiffness, giv.. |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature 23.0 °C |
1.19 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Borealis PS65T20 Polypropylene Compound, Mineral Filled PS65T20 is a 20% mineral filled polypropylene compound intended for injection and back injection molding. This material has excellent balanced mechanical properties and high melt flow rate. Applic.. |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature 23.0 °C |
1.19 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Borealis MS64T20 Polypropylene Compound, Mineral Filled MS64T20 is a 20% mineral filled polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and is easy to process. Applications: automotive p.. |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature -30.0 °C |
1.19 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
BASF Ultraform® N2520 L POM Description: Is a POM, product having reduced electric surface resistance.Information provided by BASF |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature -20.0 °C |
1.19 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PPH T8020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature -20.0 °C |
1.19 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PPH T8030 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature -20.0 °C |
1.19 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PPH TS8030 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature 23.0 °C |
1.19 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
BASF Ultramid® B3UGM210 GR 22866 10/50% Glass/Mineral Filled PA6 FR (Dry) Description: Halogen- and phosphorus-free injection-molding grade with very high rigidity, low smoke density and outstanding electrical properties.Information provided by BASF |