Techmer ES HiFill® PA6/6 GF60 IM HS L 60% Glass Filled (Conditioned)

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 60% Glass Fiber Filled , Nylon 66, Heat Stabilized
Manufacturer Techmer ES
Trade Name HiFill®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill® PA6/6 GF60 IM HS L 60% Glass Filled (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearance: Natural ColorTPCI# 8874101Information provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.67 g/cc
0.0603 lb/in³
ASTM D792
Water Absorption 0.45 %

@Time 86400 sec
0.45 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0020 cm/cm

@Thickness 3.17 mm
0.0020 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 159 MPa
23000 psi
ASTM D638
Elongation at Break 4.0 %
4.0 %
ASTM D638
Flexural Strength 241 MPa
35000 psi
ASTM D790
Flexural Modulus 11.7 GPa
1700 ksi
ASTM D790
Izod Impact, Notched 4.27 J/cm

@Thickness 3.17 mm
8.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched NB

@Thickness 3.17 mm
NB

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 257 °C
495 °F
Unannealed; ASTM D648