Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Custom Resins Norpex® 300 PPE (Polyphenylene Ether)  (discontinued **)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polyphenylene Ether, Molded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Custom Resins Norpex® 300 PPE (Polyphenylene Ether)  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Premium performance high heat. Properties for dry as molded samples.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 76.0 MPa
11000 psi
ASTM D638
Flexural Yield Strength 104 MPa
15100 psi
ASTM D790
Flexural Modulus 2.40 GPa
348 ksi
ASTM D790
Izod Impact, Notched 4.70 J/cm
8.81 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 149 °C
300 °F
ASTM D648