Material Notes:
Features:Super High ImpactExtrusionApplicationsPipeProfilesSheetInformation provided by I. Stern & Co. Inc.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Melt Flow 1.5 g/10 min
1.5 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 111
111
ASTM D785
Tensile Strength 40.1 MPa
5820 psi
ASTM D638
Elongation at Yield 70 %
70 %
ASTM D638
Flexural Strength 51.6 MPa
7480 psi
ASTM D790
Flexural Modulus 2.34 GPa
340 ksi
ASTM D790
Izod Impact, Notched 4.70 J/cm
8.80 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Heat Distortion Temperature 85.0 °C
185 °F
ASTM D648