Material Notes:
Designed for pipe and bobbin sleeves. Excellent processability and high impact strength. Manufactured to prevent static electricity.
Physical Properties Metric English Comments
Melt Flow 0.70 g/10 min
0.70 g/10 min
ASTM D1238G
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100
100
ASTM D785
Tensile Strength, Ultimate 40.0 MPa
5800 psi
ASTM D638
Elongation at Break 70 %
70 %
ASTM D638
Flexural Yield Strength 52.0 MPa
7540 psi
ASTM D790
Flexural Modulus 1.77 GPa
257 ksi
ASTM D790
Izod Impact, Notched 4.70 J/cm

@Thickness 3.17 mm
8.81 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 77.0 °C
171 °F
Heat Distortion Temp
Deflection Temperature at 1.8 MPa (264 psi) 77.0 °C
171 °F
ASTM D648
Vicat Softening Point 92.0 °C
198 °F
ASTM D1525
Flammability, UL94 HB
HB