Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.39 J/cm @Temperature 23.0 °C |
2.60 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products P250-00 Polypropylene Copolymer, Natural Applications: ConsolesComponent housingsInterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 1.39 J/cm @Temperature 23.0 °C |
2.60 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products P250-247 Polypropylene Copolymer, UV Stabilized, Black Applications: Center consolesInterior trimI/P componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 1.39 J/cm @Temperature 23.0 °C |
2.60 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products P254-00 Polypropylene Copolymer, Natural Applications: Air ducts - distributionInterior trimI/P componentsElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 1.39 J/cm @Temperature 23.0 °C |
2.60 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products P256-00 Polypropylene Copolymer, Natural Applications: Door/trunk scuffUnderhood componentsSplash shieldsElectrical enclosuresInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 1.39 J/cm | 2.60 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® C7122 PC+ABS (Asia Pacific) Cycoloy*C7122 is a mineral filled, non-halogenated flame retardant PC/ABS. Good stiffness with balanced flow and impact performance. |
|||
Izod Impact, Notched | 1.39 J/cm | 2.60 ft-lb/in | Method A; ASTM D256 |
Proto3000 ABS-M30 Fused Deposition Modeling Polymer Description: ABS-M30 is up to 25-70 percent stronger than standard Stratasys ABS and is an ideal material for conceptual modeling, functional prototyping, manufacturing tools, and end-use-parts. ABS.. |
|||
Izod Impact, Notched | 1.39 J/cm @Temperature -30.0 °C |
2.60 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HP6NR PC (Europe-Africa-Middle East) Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no .. |
|||
Izod Impact, Notched | 1.39 J/cm @Temperature -30.0 °C |
2.60 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HPS6 PC Med/low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam e-beam and gamma sterilizable. .. |
|||
Izod Impact, Notched | 1.39 J/cm @Temperature -30.0 °C |
2.60 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HPS6 PC (Europe-Africa-Middle East) Med/low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam e-beam and gamma sterilizable. .. |
|||
Izod Impact, Notched | 1.39 J/cm @Temperature -30.0 °C |
2.60 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HP6NR PC Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no .. |
|||
Izod Impact, Notched | 1.39 - 1.44 J/cm @Temperature -30.0 - -30.0 °C |
2.60 - 2.70 ft-lb/in @Temperature -22.0 - -22.0 °F |
Average value: 1.43 J/cm Grade Count:4 |
Overview of materials for Polycarbonate, Gamma Radiation Resistant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Gamma Radiation Resistant". Each property range of values reported is minimum and maximum.. |
|||
Izod Impact, Notched | 1.39 J/cm | 2.60 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP DX09407H PC LNP* LUBRICOMP* DX09407H is a compound based on High Heat Polycarbonate containing proprietary fillers. Added features of this grade are: Wear Resistant, Healthcare. |
|||
Izod Impact, Notched | 1.39 J/cm @Thickness 3.17 mm |
2.60 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6 GF43 L BK 43% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 43% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: BlackProcessing Method: Injection Mol.. |
|||
Izod Impact, Notched | 1.39 J/cm @Thickness 3.17 mm |
2.60 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6 GF44 HS L 44% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 44% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat Stabilized TPCI# 95.. |
|||
Izod Impact, Notched | 1.39 J/cm @Thickness 3.17 mm |
2.60 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/6 GF40 L 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: LubricantFeatures: LubricatedProcessing Method: Injection MoldingInformation p.. |
|||
Izod Impact, Notched | 1.39 J/cm @Thickness 3.17 mm |
2.60 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/6 GF43 L BKN001 43% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 43% Filler by WeightAdditive: Lubricant Features: Lubricated Appearance: BlackProcessing Method: Injection M.. |
|||
Izod Impact, Notched | 1.39 J/cm @Thickness 3.17 mm |
2.60 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/6 GF43 LE BK 43% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 43% Filler by WeightAdditive: Lubricant Features: Lubricated and Low ExtractablesAppearance: BlackInformatio.. |
|||
Izod Impact, Notched | 1.39 J/cm | 2.60 ft-lb/in | ASTM D256 |
Stratasys® ABS-M30i ABS-M30i is a high strength material well suited for the medical, pharmaceutical
and food packaging industries. Parts manufactured with ABS-M30i material
are biocompatible (ISO 10993 certified) an.. |
|||
Izod Impact, Notched | 1.39 J/cm | 2.60 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP RX05494 PA 66 LNP* Thermocomp* RX05494 is a compound based on Nylon 6/6 resin containing glass fiber fillers. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Notched | 1.39 J/cm | 2.60 ft-lb/in | ASTM D256 |
A. Schulman SCHULADUR® A GF20HI 20% Glass Fiber Reinforced, High Impact PBT Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.39 J/cm @Thickness 3.17 mm |
2.60 ft-lb/in @Thickness 0.125 in |
|
TPI Porene® ABS-KU650 Super High Heat ABS Resin Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 1.39 J/cm | 2.60 ft-lb/in | ASTM D256 |
Total PPC 4481WZ Polypropylene, Impact Copolymer TOTAL Petrochemicals Polypropylene 4481WZ is a nucleated impact copolymer with a Melt Flow index of 4.0 g/10 min.TOTAL Polypropylene 4481WZ is characterized by a good stiffness/impact balance couple.. |
|||
Izod Impact, Notched | 1.39 J/cm | 2.60 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Comtuf® 523 Polycarbonate/Styrenic Alloy Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc.. |
|||
Izod Impact, Notched | 1.39 J/cm | 2.60 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 625 Nylon 6/6, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.50% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Notched | 1.39 J/cm | 2.60 ft-lb/in | ASTM D256-92 |
Lubrizol Stat-Rite® M-809 Static Control Acrylic Stat-Rite® M-809 is a static dissipative Acrylic alloy. Stat-Rite® M-809 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD protec.. |