Lubrizol Stat-Rite® M-809 Static Control Acrylic

Category Polymer , Thermoplastic , Acrylic (PMMA) , Acrylic, General Purpose, Molded
Manufacturer Lubrizol (former Noveon)
Trade Name Stat-Rite®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Stat-Rite® M-809 Static Control Acrylic.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Stat-Rite® M-809 is a static dissipative Acrylic alloy. Stat-Rite® M-809 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD protection. Stat-Rite® IDP alloys provide consistent static dissipation even when extruded, injection molded or thermoformed into components. Features:Permanent static dissipative performanceHumidity insensitiveRecyclable and reusableApplications:Thermoformed packagingPCB traysElectronic component packagingProperties of all Stat-Rite® polymer products in the molten state are adversely affected by moisture. Although Stat-Rite® compounds are dry when packaged, trace amounts of moisture can be absorbed during storage and handling. For best results, always dry the material three to four hours at 70°C (160°F) in a dehumidifying hopper dryer. Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol
Physical Properties Metric English Comments
Density 1.11 g/cc
0.0401 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 26.2 MPa
3800 psi
ASTM D638
Elongation at Break 27 %
27 %
ASTM D638
Tensile Modulus 1.51 GPa
219 ksi
ASTM D638
Flexural Modulus 1.45 GPa
210 ksi
ASTM D790-92
Izod Impact, Notched 1.39 J/cm
2.60 ft-lb/in
ASTM D256-92
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °C
167 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 67.0 °C
153 °F
ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+10 ohm-cm
1.00e+10 ohm-cm
ASTM D257
Surface Resistance 9.00e+9 ohm
9.00e+9 ohm
12% RH; ESD S11.11
Surface Resistivity per Square 1.00e+10 ohm
1.00e+10 ohm
50% RH; ASTM D257
Static Decay 0.030 sec
0.030 sec
FTMS-101C; 12% R.H. (+5000 V to 50 V)
0.040 sec
0.040 sec
FTMS-101C; 12% R.H. (-5000 V to -50 V)
Descriptive Properties Value Comments
Color Transparent