Total PPC 4481WZ Polypropylene, Impact Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Sheet/Thermoforming Grade
Manufacturer Total Atofina
Trade Name PPC
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total PPC 4481WZ Polypropylene, Impact Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TOTAL Petrochemicals Polypropylene 4481WZ is a nucleated impact copolymer with a Melt Flow index of 4.0 g/10 min.TOTAL Polypropylene 4481WZ is characterized by a good stiffness/impact balance coupled with high creep resistance. This grade has been developed for sheet extrusion and thermoforming applications requiring good mechanical properties and aesthetic appearance.Total Polypropylene 4481WZ has been specially formulated with an additive for excellent antistatic properties as well as good surface appearance and mold release.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 0.905 g/cc
0.905 g/cc
ASTM D1505
Melt Flow 4.0 g/10 min
4.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 34.0 MPa
4930 psi
ASTM D638
Elongation at Yield 7.0 %
7.0 %
ASTM D638
Flexural Modulus 1.65 GPa
239 ksi
ASTM D790
Izod Impact, Notched 1.39 J/cm
2.60 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 160 - 165 °C
320 - 329 °F
DSC
Deflection Temperature at 0.46 MPa (66 psi) 115 °C
239 °F
pressure unspecified; ASTM D648