Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
Manufacturer PlastiComp
Trade Name Complēt®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PlastiComp Complet® LGF30-PBT Polybutylene Terephthalate, 30% Long Glass Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polybutylene Terephthalate (PBT) with 30% long glass fiber reinforcementInformation provided by PlastiComp, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.53 g/cc
1.53 g/cc
ASTM D-792
Filler Content 30 %
30 %
Long Glass Fiber
Mechanical Properties Metric English Comments
Tensile Strength 145 MPa
21000 psi
ASTM D-638
Elongation at Break 2.0 - 3.0 %
2.0 - 3.0 %
ASTM D-638
Tensile Modulus 10.345 GPa
1500.4 ksi
ASTM D-638
Flexural Strength 221 MPa
32100 psi
ASTM D-790
Flexural Modulus 9.655 GPa
1400 ksi
ASTM D-790
Izod Impact, Notched 2.14 J/cm
4.01 ft-lb/in
ASTM D-256
Izod Impact, Unnotched 11.75 J/cm
22.01 ft-lb/in
ASTM D-4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 204 °C
399 °F
ASTM D-648