SABIC Innovative Plastics Lexan® EXL1330 PC Copolymer

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Lexan®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Lexan® EXL1330 PC Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Lexan* EXL1330 polycarbonate (PC) siloxane copolymer resin is a UV stabilized opaque injection molding (IM) and sheet extrusion grade. This resin offers extreme low temperature (-60 C) ductility in combination with medium flow characteristics and excellent processability with opportunities for shorter IM cycle times compared to standard PC. Lexan EXL1330 resin is a general purpose product available in a wide range of opaque colors and is an excellent candidate for a broad range of applications.
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ASTM D792
Density 1.18 g/cc
0.0426 lb/in³
ISO 1183
Moisture Absorption 0.150 %
0.150 %
23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.35 %
0.35 %
ISO 62
Linear Mold Shrinkage, Flow 0.0040 - 0.0080 cm/cm

@Thickness 3.20 mm
0.0040 - 0.0080 in/in

@Thickness 0.126 in
SABIC Method
Linear Mold Shrinkage, Transverse 0.0040 - 0.0080 cm/cm

@Thickness 3.20 mm
0.0040 - 0.0080 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 10 g/10 min

@Load 1.20 kg,
Temperature 300 °C
10 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Melt Index of Compound 9.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
9.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
Mechanical Properties Metric English Comments
Hardness, H358/30 90.0 MPa
13100 psi
ISO 2039-1
Tensile Strength at Break 56.0 MPa
8120 psi
50 mm/min; ISO 527
61.0 MPa
8850 psi
Type I, 50 mm/min; ASTM D638
Tensile Strength, Yield 55.0 MPa
7980 psi
50 mm/min; ISO 527
58.0 MPa
8410 psi
Type I, 50 mm/min; ASTM D638
Elongation at Break >= 100 %
>= 100 %
50 mm/min; ISO 527
130 %
130 %
Type I, 50 mm/min; ASTM D638
Elongation at Yield 5.0 %
5.0 %
50 mm/min; ISO 527
6.0 %
6.0 %
Type I, 50 mm/min; ASTM D638
Tensile Modulus 2.10 GPa
305 ksi
50 mm/min; ASTM D638
2.10 GPa
305 ksi
1 mm/min; ISO 527
Flexural Yield Strength 85.0 MPa
12300 psi
2 mm/min; ISO 178
88.0 MPa
12800 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.06 GPa
299 ksi
1.3 mm/min, 50 mm span; ASTM D790
2.10 GPa
305 ksi
2 mm/min; ISO 178
Izod Impact, Notched 8.01 J/cm
15.0 ft-lb/in
ASTM D256
10.68 J/cm
20.01 ft-lb/in
Izod Impact, double-gated, 23°C; SABIC Method
5.87 J/cm

@Temperature -50.0 °C
11.0 ft-lb/in

@Temperature -58.0 °F
ASTM D256
6.80 J/cm

@Temperature -30.0 °C
12.7 ft-lb/in

@Temperature -22.0 °F
ASTM D256
6.40 J/cm

@Thickness 6.40 mm
12.0 ft-lb/in

@Thickness 0.252 in
ASTM D256
Izod Impact, Notched (ISO) 70.0 kJ/m²
33.3 ft-lb/in²
80*10*3; ISO 180/1A
55.0 kJ/m²

@Temperature -30.0 °C
26.2 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1A
Izod Impact, Unnotched (ISO) NB
NB
80*10*3; ISO 180/1U
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
80*10*3; ISO 180/1U
Charpy Impact Unnotched NB
NB
Edgew 80*10*3 sp=62mm; ISO 179/1eU
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 7.50 J/cm²
35.7 ft-lb/in²
Edgew 80*10*3 sp=62mm; ISO 179/1eA
6.00 J/cm²

@Temperature -30.0 °C
28.6 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 52.0 J

@Temperature 23.0 °C
38.4 ft-lb

@Temperature 73.4 °F
ASTM D3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 66.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
37.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
72.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
40.0 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
CTE, linear, Transverse to Flow 66.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
37.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
72.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
40.0 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 136 °C
277 °F
Edgew 120*10*4 sp=100mm; ISO 75/Be
134 °C

@Thickness 3.20 mm
273 °F

@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 125 °C
257 °F
Edgew 120*10*4 sp=100mm; ISO 75/Ae
120 °C

@Thickness 3.20 mm
248 °F

@Thickness 0.126 in
unannealed; ASTM D648
124 °C

@Thickness 6.40 mm
255 °F

@Thickness 0.252 in
unannealed; ASTM D648
Vicat Softening Point 143 °C
289 °F
Rate B/50; ASTM D1525
143 °C
289 °F
Rate B/50; ISO 306
145 °C
293 °F
Rate B/120; ISO 306
UL RTI, Electrical 125 °C
257 °F
UL 746B
UL RTI, Mechanical with Impact 115 °C
239 °F
UL 746B
UL RTI, Mechanical without Impact 120 °C
248 °F
UL 746B
Flammability, UL94 HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in
UL 94
Oxygen Index 35 %
35 %
ISO 4589
Glow Wire Test 875 °C
1610 °F
IEC 60695-2-13
875 °C
1610 °F
IEC 60695-2-13
850 °C

@Thickness 0.800 mm
1560 °F

@Thickness 0.0315 in
IEC 60695-2-12
960 °C

@Thickness 1.00 mm
1760 °F

@Thickness 0.0394 in
IEC 60695-2-12
Descriptive Properties Value Comments
Ball Pressure Test, 125°C +/- 2°C PASSES
IEC 60695-10-2