Polymer Property : Izod Impact, Notched = 1.20 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.500 - 1.20 J/cm
0.937 - 2.25 ft-lb/in
Average value: 0.858 J/cm Grade Count:10
Overview of materials for Polyaryletherketone (PAEK), Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Glass Fiber Filled". Each property range of values reported is minimum and m..
Izod Impact, Notched 0.370 - 1.20 J/cm
0.693 - 2.25 ft-lb/in
Average value: 0.744 J/cm Grade Count:28
Overview of materials for Polycarbonate/ABS Alloy, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Carbon Fiber Filled". Each property range of values reported is minimum and max..
Izod Impact, Notched 1.00 - 1.20 J/cm
1.87 - 2.25 ft-lb/in
ASTM D256
Loxim 140 01V0 Polycarbonate, 40% Glass Filled, Flame Retardant
Information provided by Loxim Industries
Izod Impact, Notched 1.00 - 1.20 J/cm
1.87 - 2.25 ft-lb/in
ASTM D256
Loxim 830 01 HBCC Polypropylene Compound 30% Chemically Coupled, Flame Retardant
Information provided by Loxim Industries
Izod Impact, Notched 0.400 - 1.20 J/cm

@Thickness 4.00 mm
0.749 - 2.25 ft-lb/in

@Thickness 0.157 in
ASTM D256
Solvay Specialty Polymers Solef® 6008 Polyvinylidene Fluoride (PVDF)
Solef® 6008 PVDF homopolymer is a low-viscosity PVDF resin and is typically processed by injection molding.Features: Homopolymer; Low ViscosityAdditional Properties: Crystallization Heat - ASTM D..
Izod Impact, Notched 0.600 - 1.20 J/cm

@Thickness 4.00 mm
1.12 - 2.25 ft-lb/in

@Thickness 0.157 in
ASTM D256
Solvay Specialty Polymers Solef® 9007 Polyvinylidene Fluoride (PVDF)
Solef® 9007 PVDF homopolymer has low viscosity and is used in film extrusion and injection molding.Features: Homopolymer; Low ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 53...
Izod Impact, Notched 0.700 - 1.20 J/cm
1.31 - 2.25 ft-lb/in
Average value: 1.03 J/cm Grade Count:10
Overview of materials for Polyvinyl Dichloride (PVDC)
This property data is a summary of similar materials in the MatWeb database for the category "Polyvinyl Dichloride (PVDC)". Each property range of values reported is minimum and maximum values of ap..
Izod Impact, Notched 0.300 - 1.20 J/cm

@Temperature -30.0 - -30.0 °C
0.562 - 2.25 ft-lb/in

@Temperature -22.0 - -22.0 °F
Average value: 0.567 J/cm Grade Count:122
Overview of materials for Polyetherimide (PEI)
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate Mat..