Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.534 - 1.18 J/cm | 1.00 - 2.20 ft-lb/in | Average value: 0.924 J/cm Grade Count:22 |
Overview of materials for Polyphenylene Ether, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 20% Glass Filled". Specific grades with glass content between 15% and 24% are inclu.. |
|||
Izod Impact, Notched | 0.370 - 1.18 J/cm | 0.693 - 2.21 ft-lb/in | Average value: 0.950 J/cm Grade Count:7 |
Overview of materials for Polyphenylene Ether, Glass/Graphite Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Glass/Graphite Reinforced". Each property range of values reported is minimum and m.. |