Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.540 J/cm | 1.01 ft-lb/in | ASTM D256 |
Firestone CL200-001 Nylon 6 Natural color. Not heat stabilized or modified. Lubricated. Chip size is 2 x 3.5 mm.Information provided by Firestone |
|||
Izod Impact, Notched | 0.539 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
1.01 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUCEL N145LD POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Electric/Electronic Gears, Automobile speaker HousingCAS No. 66455-31-0Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.540 J/cm | 1.01 ft-lb/in | ASTM D256 |
Kolon KOCETAL® LW301 Wear Modified Acetal Resin Special polymer added, improved wear property. Applications: Products for low noise and precision gear. Information provided by API-Kolon. |
|||
Izod Impact, Notched | 0.540 J/cm | 1.01 ft-lb/in | ASTM D256 |
Kolon KOPA® KN333HB40HFBL Hybrid Nylon 66 High flow, dimensionally stableApplications Fans & ShroudsInformation provided by API-Kolon. |
|||
Izod Impact, Notched | 0.539 J/cm | 1.01 ft-lb/in | Low Temp |
Kolon KOPEL® KP3372 General Purpose TPE Resin KOPEL® is a thermoplastic polyester elastomer which is a new engineering rubber having combined properties of conventional rubber and thermoplastic. Its flexibility and elastic recovery are very.. |
|||
Izod Impact, Notched | 0.540 J/cm | 1.01 ft-lb/in | ASTM D256 |
Kolon SPESIN® KP515FLBL High Impact PBT Alloy Resin High elastic, whether resistantApplications: WipersInformation provided by API-Kolon. |
|||
Izod Impact, Notched | 0.539 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.01 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical Lupox® GP1000H PBT Description: Injection Molding, PBT, High Flow, High ImpactApplication: Automotive (Connector)CAS No. 155123-66-3 and 24968-12-5Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.539 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.01 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical Lupox® HI2152 PBT+GF15% Description: Injection Molding, PBT+GF15%, High ImpactApplication: IT/OA, E&E (Bobbin, Switch)CAS No. 9003-01-04, 65997-17-3, 24968-12-5 and 103598-77-2Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.539 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.01 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical Lupox® SG5200 PBT+PET+GF20% Description: Injection Molding, PBT+PET+GF20%, Good Surface Application: E&E (Microwave Oven Door Gasket)CAS No. 65997-17-3, 25038-59-9 and 24968-12-5Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.539 J/cm | 1.01 ft-lb/in | ASTM D256A |
Lotte Chemical Titan TITANPRO® PM655 Polypropylene homopolymer The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1.. |
|||
Izod Impact, Notched | >= 0.539 J/cm @Thickness 6.35 mm |
>= 1.01 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Gromax PBT 1100-211H Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Izod Impact, Notched | >= 0.540 J/cm | >= 1.01 ft-lb/in | Reversed Notch (Method E); ASTM D 256 |
Karina E 854-35/1-A-ERYB Ivory PVC Compound Heavy metal free PVC compound recommended for extrusion of furniture profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Izod Impact, Notched | >= 0.540 J/cm | >= 1.01 ft-lb/in | Reversed Notch (Method E); ASTM D 256 |
Karina E 854-35/1-Y-ERYB Ivory PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Izod Impact, Notched | 0.539 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.01 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical Lupox® GP2156FT PBT+GF15% Description: Injection Molding, PBT+GF15%, Flame Retardant, High FlowApplication: IT/OA, E&E (Connector)CAS No. 71342-77-3, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical |
|||
Izod Impact, Notched | >= 0.539 J/cm @Thickness 6.35 mm |
>= 1.01 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Gromax PBT 2100-104B Product Description: PBT unreinforced flame-retarded injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excellen.. |
|||
Izod Impact, Notched | >= 0.539 J/cm @Thickness 6.35 mm |
>= 1.01 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Gromax PBT 3020-104 15% Glass Fiber Filled Product Description: A glass fiber 20% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Izod Impact, Notched | 0.540 J/cm | 1.01 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DX05301C PC LNP* STAT-KON* DX05301C is a compound based on Polycarbonate containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive, Low Ionic.. |
|||
Izod Impact, Notched | 0.540 J/cm | 1.01 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PCN2615H PPE+PS (Asia Pacific) PPE+PS, Noryl, Glass Fiber, Mica, Flame Retardant, UL Grade, Non-Halogen Flame Retaardant, High Flow, |
|||
Izod Impact, Notched | 0.540 J/cm | 1.01 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP KFI12 Acetal Copolymer LNP LUBRICOMP* KFI12 is a compound based on Acetal Copolymer resin containing 10% Glass Fiber, 2% Silicone. Added feature of this grade is: Wear Resistant. |
|||
Izod Impact, Notched | 0.539 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
1.01 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Shinkong Synthetic Fibers Shinite® E202G15 PBT, 15% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Izod Impact, Notched | 0.540 J/cm | 1.01 ft-lb/in | ASTM D256 |
UBE UBESTA® 3020X15 Nylon 12 Thermister Description: UBESTA Nylon 12 ThermisterInformation provided by UBE. |
|||
Izod Impact, Notched | 0.540 J/cm | 1.01 ft-lb/in | ASTM D256 |
UBE UBESTA® 3020X8 Nylon 12 Thermister Description: UBESTA Nylon 12 ThermisterInformation provided by UBE. |
|||
Izod Impact, Notched | 0.539 J/cm | 1.01 ft-lb/in | |
Zylog Hipolyene® 9011 UHF Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Izod Impact, Notched | 0.539 J/cm | 1.01 ft-lb/in | ASTM D256 |
Cheng Yu Plastic N6C2 Nylon 6, 20% Mineral Reinforced |
|||
Izod Impact, Notched | 0.539 J/cm | 1.01 ft-lb/in | ASTM D256 |
E-Polymers TEKAMID® TA210MS MoS2 Filled PA66 Resin Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.T-series: Impact modified,.. |
|||
Izod Impact, Notched | 0.539 J/cm | 1.01 ft-lb/in | ASTM D256 |
Aaron Industries AAROPRENE® CFPP 2040 Calcium Carbonate Filled Polypropylene AAROPRENE® CFPP 2000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified. |
|||
Izod Impact, Notched | 0.540 J/cm | 1.01 ft-lb/in | Dry; ASTM D256 |
Asahi Kasei Leona® 9400S Nylon 66 Excellent impact resistance. Suitable for thick-wall parts.Applications:Railroad tie insulatorsInformation provided by Asahi Kasei |
|||
Izod Impact, Notched | 0.540 J/cm | 1.01 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 195-N2 Acetal A general purpose, medium viscosity natural.Data provided by the manufacturer |
|||
Izod Impact, Notched | 0.540 J/cm @Temperature -40.0 °C |
1.01 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Ashley Polymers Ashlene® 279 PPO Alloy A general purpose, paintable injection molding grade with high chemical resistance and mechanical performance. Good heat resistance with dimensional stability in dark gray or black only.Data provid.. |
|||
Izod Impact, Notched | 0.540 J/cm | 1.01 ft-lb/in | ASTM D256 |
ALM PA 601-CF Filled Nylon 12 Prototyping Polymer Carbon fiber filled nylon 12 easy to process, strong light weight filled material.Low density, good dimensional stability while maintaining excellent mechanical properties.Fibers have been optimized.. |