Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kolon SPESIN® KP515FLBL High Impact PBT Alloy Resin

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Impact Grade
Manufacturer Kolon
Trade Name SPESIN®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kolon SPESIN® KP515FLBL High Impact PBT Alloy Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High elastic, whether resistantApplications: WipersInformation provided by API-Kolon.
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
ASTM D792
Moisture Absorption at Equilibrium 0.080 %
0.080 %
60% RH; ASTM D570
Linear Mold Shrinkage 0.015 - 0.019 cm/cm
0.015 - 0.019 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 114
114
ASTM D785
Tensile Strength 58.0 MPa
8410 psi
ASTM D638
Elongation at Break 25 %
25 %
ASTM D638
Flexural Strength 85.0 MPa
12300 psi
ASTM D790
Flexural Modulus 1.961 GPa
284.4 ksi
ASTM D790
Izod Impact, Notched 0.540 J/cm
1.01 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 40.0 µm/m-°C
22.2 µin/in-°F
ASTM D696
Melting Point 224 °C
435 °F
ASTM D1525
Deflection Temperature at 0.46 MPa (66 psi) 150 °C
302 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Dielectric Constant 3.7
3.7
ASTM D150
Dielectric Strength 27.0 kV/mm
686 kV/in
ASTM D149
Arc Resistance 110 sec
110 sec
ASTM D495