Material Notes:
Excellent impact resistance. Suitable for thick-wall parts.Applications:Railroad tie insulatorsInformation provided by Asahi Kasei
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
Dry; ASTM D792
Water Absorption 2.8 %
2.8 %
Wet
Mechanical Properties Metric English Comments
Hardness, Rockwell M 75
75
Dry; ASTM D785
Tensile Strength, Yield 44.0 MPa
6380 psi
Wet; ASTM D638
79.0 MPa
11500 psi
Dry; ASTM D638
Elongation at Break 60 %
60 %
Dry; ASTM D638
260 %
260 %
Wet; ASTM D638
Flexural Strength 44.0 MPa
6380 psi
Wet; ASTM D790
108 MPa
15700 psi
Dry; ASTM D790
Flexural Modulus 0.800 GPa
116 ksi
Wet; ASTM D790
2.60 GPa
377 ksi
Dry; ASTM D790
Izod Impact, Notched 0.540 J/cm
1.01 ft-lb/in
Dry; ASTM D256
2.74 J/cm
5.13 ft-lb/in
Wet; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 190 °C
374 °F
Dry; ASTM D648