Mechanical Properties Metric English Comments
Izod Impact, Notched 0.374 J/cm
0.701 ft-lb/in
ASTM D256
Ovation Polymers UTTAP QU BM513 GF BM Nylon, 13% Glass Reinforced
Glass reinforced (13 %) High Temperature Polyamide - Blow Molding grade with excellent chemical resistance, improved flow and high HDT. *All properties are measured after 48 hours of conditioning at..
Izod Impact, Notched 0.374 J/cm

@Thickness 3.18 mm
0.701 ft-lb/in

@Thickness 0.125 in
ASTM D256
LNP Emi-X® OC-1008 LEX Polyphenylene Sulfide, Carbon Fiber Reinforcement  (discontinued **)
Features: Radio Frequency Shielding, Electromagnetic Shielding, Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data ..
Izod Impact, Notched 0.374 J/cm
0.701 ft-lb/in
ASTM D256
LNP NORYL® EXCP0111 PPS + Polyphenylene Ether, 42% Glass / Mineral Reinforcement  (discontinued **)
For applications requiring voltage resistance.Features: Corona resistantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labele..
Izod Impact, Notched 0.374 J/cm

@Thickness 3.18 mm
0.701 ft-lb/in

@Thickness 0.125 in
ASTM D256
LNP Stat-Kon® LC-1003 EM Polyetheretherketone, Carbon Fiber Reinforcement  (discontinued **)
Features: Good Moldability, Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; howev..
Izod Impact, Notched 0.374 J/cm

@Thickness 3.18 mm
0.701 ft-lb/in

@Thickness 0.125 in
ASTM D256
LNP Thermocomp® JF-1004 EM M BK905 Polyethersulfone, Milled Glass Fiber  (discontinued **)
Features: Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are st..
Izod Impact, Notched 0.374 - 0.374 J/cm

@Temperature -30.0 - -30.0 °C
0.701 - 0.701 ft-lb/in

@Temperature -22.0 - -22.0 °F
Average value: 2.37 J/cm Grade Count:1
Overview of materials for Polycarbonate/ASA Alloy, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ASA Alloy, Unreinforced". Each property range of values reported is minimum and maximum va..
Izod Impact, Notched 0.374 - 0.374 J/cm

@Thickness 3.17 - 3.17 mm
0.701 - 0.701 ft-lb/in

@Thickness 0.125 - 0.125 in
Average value: 2.37 J/cm Grade Count:1
Overview of materials for Polycarbonate/ASA Alloy, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ASA Alloy, Unreinforced". Each property range of values reported is minimum and maximum va..
Izod Impact, Notched 0.374 J/cm
0.701 ft-lb/in
ASTM D256
LNP ULTEM® SMU5872 Polyetherimide, 25% PTFE Lubricant  (discontinued **)
Not stand-alone resin: Compounding/ concentrate for wear resistance. Will be commercialized as UF2500.Features: Lubricated, Good Wear ResistanceForms: PelletsInformation provided by LNP, a GE Plasti..
Izod Impact, Notched 0.374 J/cm
0.701 ft-lb/in
ASTM D256
Sumitomo Bakelite Durez® 32245 Phenolic, Compression Grade
Durez 32245 Black Phenolic is a two-stage glass fiber and mineral filled special purpose molding compound. It is especially designed for applications requiring high strength and dimensional stabilit..
Izod Impact, Notched 0.374 J/cm
0.701 ft-lb/in
ASTM D256A
Total PPH 3230 Polypropylene, Blow Molding Grade
Homopolymer blow molding gradeLubricated - Fina 3230 offers superior core rod release, eliminating the need for additional lubricant.High Purity - Fina 3230 features minimum taste and odor and optim..
Izod Impact, Notched 0.374 J/cm
0.701 ft-lb/in
ASTM D256A
Total PPR 3230XZ Polypropylene, Blow Molding Grade
Homopolymer Blow Molding GradeLubricated – FINA 3230XZ offers superior core road release, eliminating the need for additional lubricant.Antistat – FINA 3230XZ contains antistat to minimize dust ac..
Izod Impact, Notched 0.374 J/cm
0.701 ft-lb/in
ASTM D256A
Dow NRD6-589 Polypropylene Random Copolymer Resin
DOW NRD6-589 Polypropylene Resin is intended for use in injection molding applications. It offers excellent balance of impact and stiffness.Consistent processabilityGood stiffness/impact balanceGoo..
Izod Impact, Notched 0.374 J/cm
0.701 ft-lb/in
ASTM D256A
Braskem INSPIRE™ 404 Performance Polypropylene Polymer
INSPIRE 404 Performance Polymer is a propylene-based resin intended for use in thermoforming applications where exceptional stiffness, clarity and heat resistance is desired. The high stiffness of ..
Izod Impact, Notched 0.374 J/cm
0.701 ft-lb/in
ASTM D256
LNP ULTEM® SMU5831 Polyetherimide, 30% CarbonGlassMineral Reinforced  (discontinued **)
ESD characteristics for ultra high-heat applications. Will be UC3010H.Features: High Heat ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Compa..
Izod Impact, Notched 0.374 J/cm
0.701 ft-lb/in
ASTM D256
LNP ULTEM® SMU5832 Polyetherimide, 30% CarbonGlassMineral Reinforced  (discontinued **)
ESD characteristics for ultra high-heat applications. Will be UC3010.Features: High Heat ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Compan..
Izod Impact, Notched 0.374 J/cm

@Thickness 3.18 mm
0.701 ft-lb/in

@Thickness 0.125 in
ASTM D256
LNP Lubricomp® OCL-4536 Polyphenylene Sulfide, Carbon Fiber Reinforced, PTFE + Silicone Lubricant  (discontinu
Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac..