Braskem INSPIRE™ 404 Performance Polypropylene Polymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Sheet/Thermoforming Grade
Manufacturer Braskem
Trade Name INSPIRE™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem INSPIRE™ 404 Performance Polypropylene Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
INSPIRE 404 Performance Polymer is a propylene-based resin intended for use in thermoforming applications where exceptional stiffness, clarity and heat resistance is desired. The high stiffness of the resin may allow for the potential to down gauge and reduce part weight. The product is well suited for thin wall containers, serviceware and closure applications such as clear drink cups, deli containers, take-out containers, bowls and clear lids.Main CharacteristicsContains a nucleating agentExcellent balance of stiffness and claritySuperior heat resistance over conventional polypropyleneComplies with U.S. FDA 21 CFR 117.1520(c)3.2a (with Restrictions)Canadian HPFB No ObligationThis product line was spun off from Dow Chemical to Braskem
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Index of Compound 3.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 42.1 MPa
6110 psi
ASTM D638
Flexural Modulus, 1% Secant 2070 MPa
300000 psi
ASTM D790B
Izod Impact, Notched 0.374 J/cm
0.701 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 129 °C
264 °F
Unannealed; ASTM D648
Optical Properties Metric English Comments
Haze 16 %
16 %
1000 microns; ASTM D1003