Lucent Polymers PBT-FR310 Polybutylene Terephthalate, Flame Resistant

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Flame Retardant
Manufacturer Lucent Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucent Polymers PBT-FR310 Polybutylene Terephthalate, Flame Resistant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.37 g/cc
1.37 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.016 cm/cm

@Thickness 3.17 mm
0.016 in/in

@Thickness 0.125 in
1/8" Section
Mechanical Properties Metric English Comments
Tensile Strength, Yield 58.62 MPa
8502 psi
ASTM D638
Elongation at Break >= 8.0 %
>= 8.0 %
ASTM D638
Flexural Strength 82.76 MPa
12000 psi
ASTM D790
Flexural Modulus 2.759 GPa
400.1 ksi
ASTM D790
Izod Impact, Notched 0.320 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
0.600 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 71.11 °C
160.0 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 3.17 mm
V-0

@Thickness 0.125 in