Mechanical Properties Metric English Comments
Izod Impact, Notched 0.299 J/cm
0.560 ft-lb/in
ASTM D256
LyondellBasell Alathon® H5642 High Density Polyethylene, Injection Molding Grade  (discontinued **)
ALATHON H5642 is a multi-purpose, narrow molecular weight distribution high-flow resin featuring enhanced processing and thermal stability for fast cycling. This resin exhibits good color and organo..
Izod Impact, Notched 0.299 J/cm

@Temperature 23.0 °C
0.560 ft-lb/in

@Temperature 73.4 °F
ASTM D256
LyondellBasell Alathon® H4262 High Density Polyethylene, Injection Molding Grade  (discontinued **)
ApplicationsAlathon H4262 is a high-flow resin that exhibits very good cold temperature impact performance, optimum processing and thermal stability, with good color and organoleptic properties. Typ..
Izod Impact, Notched 0.299 J/cm
0.560 ft-lb/in
ASTM D256
LyondellBasell Alathon® H5112 High Density Polyethylene, Injection Molding Grade
ALATHON H5112 is a medium-molecular-weight-distribution resin with balanced impact/ESCR and high flow characteristics. Typical applications include housewares, food containers, pail handles and toys..
Izod Impact, Notched 0.299 J/cm
0.560 ft-lb/in
ASTM D256
Sumitomo Bakelite Sumikon® PM-9501 Glass-Filled Phenolic, Compression Grade
Sumikon PM-9501 is a two stage glass fiber and mineral filled black phenolic special purpose molding compound. It is especially designed for applications requiring high strength and dimensional s..
Izod Impact, Notched 0.299 J/cm
0.560 ft-lb/in
ASTM D256
Aclo Accutech Polypropylene Homopolymer HP0334T30L Talc Reinforced
Izod Impact, Notched 0.299 J/cm
0.560 ft-lb/in
ASTM D256
Aclo Accutech Polypropylene Homopolymer HP0334T40L Talc Reinforced
Izod Impact, Notched 0.299 J/cm
0.560 ft-lb/in
ASTM D256
Aclo Accutech Polypropylene Homopolymer HP0334T40L1 Talc Reinforced
Izod Impact, Notched 0.299 J/cm
0.560 ft-lb/in
ASTM D256
Aclo Accutech Polypropylene Homopolymer HP0336M40CL Mica Reinforced Coupled
Izod Impact, Notched 0.299 J/cm
0.560 ft-lb/in
ASTM D256
Aclo Accutech Polypropylene Homopolymer HP0336T10L1 Talc Reinforced
Izod Impact, Notched 0.299 J/cm
0.560 ft-lb/in
ASTM D256
Aclo Accutech Polypropylene Homopolymer HP0336T20L Talc Reinforced
Izod Impact, Notched 0.299 J/cm
0.560 ft-lb/in
ASTM D256
Aclo Accutech Polypropylene Homopolymer HP0336T20L1 Talc Reinforced
Izod Impact, Notched 0.299 J/cm
0.560 ft-lb/in
ASTM D256
Aclo Accutech Polypropylene Homopolymer HP0336T30L Talc Reinforced
Izod Impact, Notched 0.299 J/cm
0.560 ft-lb/in
ASTM D256
Aclo Accutech Polypropylene Homopolymer HP0336T30L1 Talc Reinforced
Izod Impact, Notched 0.299 J/cm
0.560 ft-lb/in
ASTM D256
Aclo Accutech Polypropylene Homopolymer HP0336T40L Talc Reinforced
Izod Impact, Notched 0.299 J/cm
0.560 ft-lb/in
ASTM D256
Aclo Accutech Polypropylene Homopolymer HP0336T40L1 Talc Reinforced
Izod Impact, Notched 0.299 J/cm
0.560 ft-lb/in
ASTM D256
Aclo Accutech Polypropylene Homopolymer HP0336W40L Wollastonite Reinforced
Izod Impact, Notched 0.299 J/cm
0.560 ft-lb/in
ASTM D256
Aclo Accutech Polypropylene Homopolymer HP0339G10CL Glass Reinforced Coupled
Izod Impact, Notched 0.299 J/cm
0.560 ft-lb/in
ASTM D256
Aclo Accutech Polypropylene Homopolymer HP0339W20L Wollastonite Reinforced
Izod Impact, Notched 0.299 J/cm
0.560 ft-lb/in
ASTM D256
Aclo Accutech Polypropylene Homopolymer HP0339W40L Wollastonite Reinforced
Izod Impact, Notched 0.299 J/cm
0.560 ft-lb/in
Abatron AboCast 7703-21/AboCure 7703-22 (B) Epoxy Adhesive and Casting Compound
AboCast 7703-21/AboCure 7703-21 is an all-purpose clear, low-viscosity, variable-ratio epoxy adhesive and casting compound for electric and structural applications. As an Adhesive: it bonds permane..
Izod Impact, Notched 0.299 J/cm
0.560 ft-lb/in
ASTM D256
Aclo Accucomp Polypropylene HPO306L Homopolymer
Izod Impact, Notched 0.299 J/cm
0.560 ft-lb/in
ASTM D256
Aclo Accutech Polypropylene Homopolymer HP0339M40L Mica Reinforced
Izod Impact, Notched 0.299 J/cm
0.560 ft-lb/in
ASTM D256
Aclo Accutech Polypropylene Homopolymer HP0339T10L Talc Reinforced
Izod Impact, Notched 0.299 J/cm
0.560 ft-lb/in
ASTM D256
Aclo Accutech Polypropylene Homopolymer HP0339W10L Wollastonite Reinforced
Izod Impact, Notched 0.299 J/cm
0.560 ft-lb/in
ASTM D256
Aclo Accutech Polypropylene Homopolymer HP0339W30L Wollastonite Reinforced
Izod Impact, Notched 0.299 J/cm
0.560 ft-lb/in
ASTM D256
BCC Products EB 6200 Epoxy Tooling Board
EB6200 is a “grain-free” elevated temperature epoxy modeling material known for its superior surface finish, dimensional stability and the ability to maintain tolerances even after being subjected..
Izod Impact, Notched 0.299 - 21.0 J/cm
0.560 - 39.3 ft-lb/in
Average value: 10.9 J/cm Grade Count:4