Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.299 J/cm | 0.560 ft-lb/in | ASTM D256 |
LyondellBasell Alathon® H5642 High Density Polyethylene, Injection Molding Grade
(discontinued **) ALATHON H5642 is a multi-purpose, narrow molecular weight distribution high-flow resin featuring enhanced processing and thermal stability for fast cycling. This resin exhibits good color and organo.. |
|||
Izod Impact, Notched | 0.299 J/cm @Temperature 23.0 °C |
0.560 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LyondellBasell Alathon® H4262 High Density Polyethylene, Injection Molding Grade
(discontinued **) ApplicationsAlathon H4262 is a high-flow resin that exhibits very good cold temperature impact performance, optimum processing and thermal stability, with good color and organoleptic properties. Typ.. |
|||
Izod Impact, Notched | 0.299 J/cm | 0.560 ft-lb/in | ASTM D256 |
LyondellBasell Alathon® H5112 High Density Polyethylene, Injection Molding Grade ALATHON H5112 is a medium-molecular-weight-distribution resin with balanced impact/ESCR and high flow characteristics. Typical applications include housewares, food containers, pail handles and toys.. |
|||
Izod Impact, Notched | 0.299 J/cm | 0.560 ft-lb/in | ASTM D256 |
Sumitomo Bakelite Sumikon® PM-9501 Glass-Filled Phenolic, Compression Grade Sumikon PM-9501 is a two stage glass fiber and mineral filled black phenolic special purpose molding compound. It is especially designed for applications requiring high strength and dimensional s.. |
|||
Izod Impact, Notched | 0.299 J/cm | 0.560 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0334T30L Talc Reinforced |
|||
Izod Impact, Notched | 0.299 J/cm | 0.560 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0334T40L Talc Reinforced |
|||
Izod Impact, Notched | 0.299 J/cm | 0.560 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0334T40L1 Talc Reinforced |
|||
Izod Impact, Notched | 0.299 J/cm | 0.560 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0336M40CL Mica Reinforced Coupled |
|||
Izod Impact, Notched | 0.299 J/cm | 0.560 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0336T10L1 Talc Reinforced |
|||
Izod Impact, Notched | 0.299 J/cm | 0.560 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0336T20L Talc Reinforced |
|||
Izod Impact, Notched | 0.299 J/cm | 0.560 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0336T20L1 Talc Reinforced |
|||
Izod Impact, Notched | 0.299 J/cm | 0.560 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0336T30L Talc Reinforced |
|||
Izod Impact, Notched | 0.299 J/cm | 0.560 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0336T30L1 Talc Reinforced |
|||
Izod Impact, Notched | 0.299 J/cm | 0.560 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0336T40L Talc Reinforced |
|||
Izod Impact, Notched | 0.299 J/cm | 0.560 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0336T40L1 Talc Reinforced |
|||
Izod Impact, Notched | 0.299 J/cm | 0.560 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0336W40L Wollastonite Reinforced |
|||
Izod Impact, Notched | 0.299 J/cm | 0.560 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0339G10CL Glass Reinforced Coupled |
|||
Izod Impact, Notched | 0.299 J/cm | 0.560 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0339W20L Wollastonite Reinforced |
|||
Izod Impact, Notched | 0.299 J/cm | 0.560 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0339W40L Wollastonite Reinforced |
|||
Izod Impact, Notched | 0.299 J/cm | 0.560 ft-lb/in | |
Abatron AboCast 7703-21/AboCure 7703-22 (B) Epoxy Adhesive and Casting Compound AboCast 7703-21/AboCure 7703-21 is an all-purpose clear, low-viscosity, variable-ratio epoxy adhesive and casting compound for electric and structural applications. As an Adhesive: it bonds permane.. |
|||
Izod Impact, Notched | 0.299 J/cm | 0.560 ft-lb/in | ASTM D256 |
Aclo Accucomp Polypropylene HPO306L Homopolymer |
|||
Izod Impact, Notched | 0.299 J/cm | 0.560 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0339M40L Mica Reinforced |
|||
Izod Impact, Notched | 0.299 J/cm | 0.560 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0339T10L Talc Reinforced |
|||
Izod Impact, Notched | 0.299 J/cm | 0.560 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0339W10L Wollastonite Reinforced |
|||
Izod Impact, Notched | 0.299 J/cm | 0.560 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0339W30L Wollastonite Reinforced |
|||
Izod Impact, Notched | 0.299 J/cm | 0.560 ft-lb/in | ASTM D256 |
BCC Products EB 6200 Epoxy Tooling Board EB6200 is a “grain-free” elevated temperature epoxy modeling material known for its superior surface finish, dimensional stability and the ability to maintain tolerances even after being subjected.. |
|||
Izod Impact, Notched | 0.299 - 21.0 J/cm | 0.560 - 39.3 ft-lb/in | Average value: 10.9 J/cm Grade Count:4 |
Overview of materials for Epoxy Molding Compound This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Molding Compound". Each property range of values reported is minimum and maximum values of appropr.. |