Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Formosa Plastics Formolene® 4101O BCF Fiber Spinning Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Fiber Grade
Manufacturer Formosa Plastics Corporation, USA
Trade Name Formolene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Formosa Plastics Formolene® 4101O BCF Fiber Spinning Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HomopolymerApplications: Multifilament and bulk continuous filament fiber.Formolene 4101O is a low viscosity, highly isotactic polypropylene homopolymer designed primarily for multifilament and bulk continuous filament fiber. It contains a unique combination of stabilizers which give it excellent gas fading resistance, mild UV resistance and appropriate process stability.Specimens were injection molded according to the conditions specified in ASTM D4101.Information provided by Formosa Plastics Corporation, USA.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 19 g/10 min

@Temperature 230 °C
19 g/10 min

@Temperature 446 °F
I<sub>2</sub>; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105
105
ASTM D785
Tensile Strength, Yield 34.5 MPa
5000 psi
2" (50mm) per min.; ASTM D638
Elongation at Yield 9.0 %
9.0 %
2" (50mm) per min.; ASTM D638
Flexural Modulus 1.38 GPa
200 ksi
1.3mm per min, 1% secant; ASTM D790
Izod Impact, Notched 0.267 J/cm
0.500 ft-lb/in
ASTM D256