Asahi Kasei Thermylene® P-20TC-5100 Chemically Coupled Polypropylene Compound, 20% Talc Filled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Talc Filler
Manufacturer Asahi Kasei
Trade Name Thermylene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Asahi Kasei Thermylene® P-20TC-5100 Chemically Coupled Polypropylene Compound, 20% Talc Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Automotive: Blower Wheels, HVAC Electrical and Specialty: Flush Valves, Pump BasesInformation provided by Asahi Kasei
Physical Properties Metric English Comments
Melt Flow 6.0 g/10 min
6.0 g/10 min
Mechanical Properties Metric English Comments
Tensile Strength, Yield 32.4 MPa
4700 psi
Elongation at Yield 30 %
30 %
Flexural Modulus 2.14 GPa
310 ksi
Izod Impact, Notched 0.267 J/cm
0.500 ft-lb/in
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 130 °C
266 °F
Flammability, UL94 HB
HB