Polymer Property : Izod Impact, Notched = 6.90 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.267 - 6.90 J/cm
0.500 - 12.9 ft-lb/in
Average value: 0.806 J/cm Grade Count:159
Overview of materials for Polysulfone (PSU)
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb..