Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chase Plastics CP Pryme® N100HL (Dry) Nylon 6, Heat Stabilized, Lubricated

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Heat Stabilized
Manufacturer Chase Plastics
Trade Name CP Pryme®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chase Plastics CP Pryme® N100HL (Dry) Nylon 6, Heat Stabilized, Lubricated.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Heat stabilizedLubricatedForm: PelletsInformation provided by Chase Plastics.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Water Absorption 1.6 %
1.6 %
At 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0090 - 0.013 cm/cm
0.0090 - 0.013 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength at Break 82.7 MPa
12000 psi
ASTM D638
Elongation at Break 10 %
10 %
ASTM D638
Flexural Strength 110 MPa
16000 psi
ASTM D790
Flexural Modulus 3.17 GPa
460 ksi
ASTM D790
Izod Impact, Notched 0.427 J/cm
0.800 ft-lb/in
0.125 in; ASTM D256
Thermal Properties Metric English Comments
Melting Point 216 °C
420 °F
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C
158 °F
Unannealed; ASTM D648
Copyright © lookpolymers.com All Rights Reserved