Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Asahi Kasei Thermofil P-10CC-1417 10% Calcium Carbonate Reinforced, Heat Stabilized

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 10% Calcium Carbonate (CaCO3) Filler
Manufacturer Asahi Kasei
Trade Name Thermofil
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Asahi Kasei Thermofil P-10CC-1417 10% Calcium Carbonate Reinforced, Heat Stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Asahi Thermofil
Physical Properties Metric English Comments
Specific Gravity 0.980 g/cc
0.980 g/cc
ASTM D792
Linear Mold Shrinkage 0.016 cm/cm
0.016 in/in
ASTM D955
Melt Flow 6.0 g/10 min
6.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 70
70
ASTM D785
Tensile Strength, Yield 29.0 MPa
4200 psi
ASTM D638
Elongation at Yield 100 %
100 %
ASTM D638
Flexural Strength 42.7 MPa
6200 psi
ASTM D790
Flexural Modulus 1.31 GPa
190 ksi
ASTM D790
Izod Impact, Notched 0.427 J/cm
0.800 ft-lb/in
ASTM D256
Izod Impact, Unnotched 5.34 J/cm
10.0 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 90.6 °C
195 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 68.3 °C
155 °F
ASTM D648