Mechanical Properties Metric English Comments
Izod Impact, Notched 0.110 - 0.160 J/cm
0.206 - 0.300 ft-lb/in
ASTM D256
Proto3000 Accura® 45HC Plastic Stereolithography (SLA) Prototyping Polymer
A high speed material, with excellent thermal and moisture resistance for producing functional prototypes in 3D Systems' SLA 250 systems.Benefits:Fast build speed:Provides build speeds that are sign..
Izod Impact, Notched <= 0.110 J/cm
<= 0.206 ft-lb/in
ASTM D256
Proto3000 CastForm™ PS Selective Laser Sintering (SLS®) Prototyping Polymer
Description: Directly produce complex investment casting patterns without tooling..Features: Functions like foundry wax and is “foundry friendly”Low residual ash content (less than 0.02%)Short bur..
Izod Impact, Notched 0.110 J/cm
0.206 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP LUBRICOMP BX02715 SAN
LNP* LUBRICOMP* BX02715 is a compound based on SAN containing proprietary fillers. Added features of this grade include: Wear Resistant, Tight Dimensional Tolerance, Good for Water Meter Applicati..
Izod Impact, Notched 0.110 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
0.206 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D256
IRPC Polimaxx Polene HI650 Polystyrene
APPLICATIONS: INJECTION MOULDING, ELECTRICAL APPLIANCES, HOUSEHOLD PRODUCT, TOYS, SANITARY WARES. etc.
Izod Impact, Notched 0.110 - 0.160 J/cm
0.206 - 0.300 ft-lb/in
ASTM D256
3D Systems Accura® 45HC Plastic for SLA® Systems
A high speed material, with excellent thermal and moisture resistance for producing functional prototypes in 3D Systems' SLA 250 systems.ApplicationsHigh temperature testing:Automotive "under-the-ho..
Izod Impact, Notched 0.110 J/cm
0.206 ft-lb/in
ASTM D256
ALM PS 200 Prototyping Polymer
Non-spherical polystyrene powder for production of complex investment casting patterns.PS-200 can be used as a direct drop in replacement for Castform®, and can be successfully blended with Castfor..
Izod Impact, Notched 0.110 J/cm

@Thickness 3.20 mm
0.206 ft-lb/in

@Thickness 0.126 in
ASTM D256
Beijing Chemical Industry KAIFA® GL3200 ABS Flame-Retardant Grade
Good flammabilityInformation provided by Beijing Chemical Industry Research Institute (Group)
Izod Impact, Notched <= 0.110 J/cm
<= 0.206 ft-lb/in
ASTM D256
3D Systems CastForm™ PS Plastic for SLS® Systems
For use with all selective laser sintering (SLS®) systems.ApplicationsCreate patterns directly rather than through indirect methodsComplex investment casting patternsReactive metals like titaniumLo..
Izod Impact, Notched 0.110 J/cm

@Temperature 23.0 °C
0.206 ft-lb/in

@Temperature 73.4 °F
ASTM D256
LATI LARTON CE/60 60% Special Mineral Filled Polyphenylene sulfide (PPS)  (Unverified Data**)
Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex..
Izod Impact, Notched 0.110 J/cm

@Temperature 23.0 °C
0.206 ft-lb/in

@Temperature 73.4 °F
ASTM D256A
Braskem H 152 Fiber Extrusion Polypropylene
Applications: Nonwoven by blow process for disposable diapers, personal care and disposable medical care. Information provided by Braskem
Izod Impact, Notched 0.110 - 5340 J/cm
0.206 - 10000 ft-lb/in
Average value: 0.756 J/cm Grade Count:109
Overview of materials for Polypropylene, Extrusion Grade