Braskem H 152 Fiber Extrusion Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Extrusion Grade
Manufacturer Braskem
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem H 152 Fiber Extrusion Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Nonwoven by blow process for disposable diapers, personal care and disposable medical care. Information provided by Braskem
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM D792A
Melt Flow 1100 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1100 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238L
Mechanical Properties Metric English Comments
Hardness, Rockwell R 98
98
ASTM D785
Flexural Modulus 1.40 GPa
203 ksi
ASTM D790
Izod Impact, Notched 0.110 J/cm

@Temperature 23.0 °C
0.206 ft-lb/in

@Temperature 73.4 °F
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 98.0 °C
208 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 58.0 °C
136 °F
ASTM D648
Vicat Softening Point 149 °C
300 °F
-1kg; ASTM D1525