Material Notes:
LNP* LUBRICOMP* BX02715 is a compound based on SAN containing proprietary fillers. Added features of this grade include: Wear Resistant, Tight Dimensional Tolerance, Good for Water Meter Applications.
Physical Properties Metric English Comments
Specific Gravity 1.34 g/cc
1.34 g/cc
ASTM D792
Density 1.35 g/cc
0.0488 lb/in³
ASTM D792
1.35 g/cc
0.0488 lb/in³
ISO 1183
Moisture Absorption 0.110 %
0.110 %
50% RH, 24 hrs; ASTM D570
0.150 %
0.150 %
23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm

@Time 86400 sec
0.0020 - 0.0040 in/in

@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.0030 - 0.0050 cm/cm

@Time 86400 sec
0.0030 - 0.0050 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 58.0 MPa
8410 psi
5 mm/min; ISO 527
60.0 MPa
8700 psi
Type I, 5 mm/min; ASTM D638
Elongation at Break 1.0 %
1.0 %
5 mm/min; ISO 527
1.1 %
1.1 %
Type I, 5 mm/min; ASTM D638
Tensile Modulus 8.46 GPa
1230 ksi
1 mm/min; ISO 527
9.18 GPa
1330 ksi
5 mm/min; ASTM D638
Flexural Strength 71.0 MPa
10300 psi
ISO 178
87.0 MPa
12600 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 7.97 GPa
1160 ksi
2 mm/min; ISO 178
8.10 GPa
1170 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 0.110 J/cm
0.206 ft-lb/in
ASTM D256
Izod Impact, Unnotched 0.830 J/cm
1.55 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 1.00 kJ/m²
0.476 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 6.00 kJ/m²
2.86 ft-lb/in²
80*10*4; ISO 180/1U
Dart Drop, Total Energy 3.00 J

@Temperature 23.0 °C
2.21 ft-lb

@Temperature 73.4 °F
ASTM D3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 39.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
21.7 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
CTE, linear, Transverse to Flow 45.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
25.0 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 101 °C
214 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
101 °C

@Thickness 3.20 mm
214 °F

@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 96.0 °C
205 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
96.0 °C

@Thickness 3.20 mm
205 °F

@Thickness 0.126 in
unannealed; ASTM D648
Copyright © lookpolymers.com All Rights Reserved