Material Notes:
Description: Directly produce complex investment casting patterns without tooling..Features: Functions like foundry wax and is “foundry friendly”Low residual ash content (less than 0.02%)Short burnout cycleEasy-to-process plasticGood plastic powder recycle characteristicsBenefits:Create complex patterns without welds or jointsReduce lead times resulting in faster time-to-marketCompatible with autoclaves, low-temperature furnaces, and vacuum plaster casting methodsEasy to assemble and repair patternsRapidly test new designs in iterative processApplications: Create patterns directly rather than through indirect methodsComplex investment casting patterns- Reactive metals like titanium- Low melt-temperature metals such as aluminum, magnesium and zinc- Ferrous and non-ferrous metalsEconomic, low-volume production castings without toolingSmaller parts can be joined to create very large patternsSacrificial, expendable patternsCastform™ PS patterns are comparable to conventional wax patterns in the following areas:Assembly methods and toolsStability and transportabilityHandling during assembly and repairSuitable for all cast metal alloysLow residual ashNo ceramic shell crackingUsable for ceramic and plaster moldsInformation provided by Proto3000 for their protoyping engineering services.
Physical Properties Metric English Comments
Density 0.460 g/cc
0.0166 lb/in³
tap; ASTM D4164
0.860 g/cc
0.0311 lb/in³
ASTM D792
Moisture Absorption at Equilibrium 0.060 %

@Temperature 20.0 °C
0.060 %

@Temperature 68.0 °F
65% RH; ASTM D570
Ash 0.020 %
0.020 %
ASTM D482
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 2.84 MPa
412 psi
ASTM D638
Tensile Modulus 1.604 GPa
232.6 ksi
ASTM D638
Izod Impact, Notched <= 0.110 J/cm
<= 0.206 ft-lb/in
ASTM D256
Izod Impact, Unnotched 0.140 J/cm
0.262 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 89.0 °C
192 °F
Polystyrene; ASTM D3418
Flash Point >= 200 °C
>= 392 °F
Wax
350 °C
662 °F
Polystyrene Method
Descriptive Properties Value Comments
Autoignition Point 410°C
Polystyrene
Upward Surface 13 µm
as processed, Mitutoyo Surftest-402
3 µm
after polishing, Mitutoyo Surftest-402