ALM PS 200 Prototyping Polymer

Category Polymer , Rapid Prototyping Polymer , Thermoplastic , Polystyrene (PS)
Manufacturer ALM Advanced Laser Materials
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ALM PS 200 Prototyping Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Non-spherical polystyrene powder for production of complex investment casting patterns.PS-200 can be used as a direct drop in replacement for Castform®, and can be successfully blended with Castform® without any change in processing parameters.Optimized for Sinterstation platforms.Infiltrated with Red Wax #2-D504Information provided by Advanced Laser Materials (ALM).
Physical Properties Metric English Comments
Bulk Density 0.460 g/cc
0.0166 lb/in³
ASTM D1895
Density 0.860 g/cc
0.0311 lb/in³
Sintered; ASTM D792
Ash 0.020 %
0.020 %
ASTM D482
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 2.84 MPa
412 psi
Infiltrated; ASTM D638
Tensile Modulus 1.604 GPa
232.6 ksi
Infiltrated; ASTM D638
Izod Impact, Notched 0.110 J/cm
0.206 ft-lb/in
ASTM D256
Izod Impact, Unnotched 0.140 J/cm
0.262 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point >= 63.0 °C
>= 145 °F
Wax Infiltrated; ASTM D3418
Glass Transition Temp, Tg 89.0 °C
192 °F
Unifiltrated; ASTM D3418