Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.200 - 0.680 J/cm² | 0.952 - 3.24 ft-lb/in² | Average value: 0.424 J/cm² Grade Count:15 |
Overview of materials for Acetal Copolymer, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Mineral Filled". Each property range of values reported is minimum and maximum values .. |
|||
Charpy Impact, Notched | 0.600 - 0.680 J/cm² @Temperature -20.0 - -20.0 °C |
2.86 - 3.24 ft-lb/in² @Temperature -4.00 - -4.00 °F |
Average value: 0.616 J/cm² Grade Count:5 |
Overview of materials for Polycarbonate, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E.. |