Material Notes:
Coextrusion grade developed to provide high aesthetic control, outstanding weatherability and impact and scratch resistance, the Elvakon® series enables protection of substrates with a durable protective coating.Information provided by Lucite International
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
ISO 1183
Water Absorption 0.35 %
0.35 %
ISO 62
Melt Flow 2.9 g/10 min
2.9 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell M 48
48
ISO 2039-2
Tensile Strength 50.0 MPa
7250 psi
ISO 527
Elongation at Break 25 %
25 %
ISO 527
Flexural Strength 67.0 MPa
9720 psi
ISO 178
Flexural Modulus 2.10 GPa
305 ksi
ISO 178
Izod Impact, Notched (ISO) 6.10 kJ/m²
2.90 ft-lb/in²
ISO 180/1A
Charpy Impact, Notched 0.600 J/cm²
2.86 ft-lb/in²
ISO 179/1eA
6.40 J/cm²
30.5 ft-lb/in²
ISO 179/1eU
Thermal Properties Metric English Comments
Vicat Softening Point 91.0 °C
196 °F
ISO 306B
102 °C
216 °F
ISO 306A
Heat Distortion Temperature 90.0 °C
194 °F
ISO 75A
Optical Properties Metric English Comments
Refractive Index 1.49
1.49
ISO 489
Transmission, Visible 90 %
90 %
ASTM D1003