LATI Latamid 66 MDT05-01 PA 66

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer LATI
Trade Name Latamid
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LATI Latamid 66 MDT05-01 PA 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polyamide 66 (PA66) based compound. Magnetic detectable filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0491 lb/in³
Linear Mold Shrinkage, Flow 0.0060 - 0.010 cm/cm
0.0060 - 0.010 in/in
Linear Mold Shrinkage, Transverse 0.0060 - 0.010 cm/cm
0.0060 - 0.010 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 55.0 MPa

@Temperature 23.0 °C
7980 psi

@Temperature 73.4 °F
Elongation at Break 12 %

@Temperature 23.0 °C
12 %

@Temperature 73.4 °F
Elongation at Yield 5.0 %
5.0 %
Tensile Modulus 2.80 GPa

@Temperature 23.0 °C
406 ksi

@Temperature 73.4 °F
Charpy Impact Unnotched NB
NB
Charpy Impact, Notched 0.600 J/cm²
2.86 ft-lb/in²
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 250 °C
482 °F
Deflection Temperature at 1.8 MPa (264 psi) 230 °C
446 °F
Vicat Softening Point 250 °C

@Load 5.00 kg
482 °F

@Load 11.0 lb
Processing Properties Metric English Comments
Melt Temperature 270 - 290 °C
518 - 554 °F
Mold Temperature 80.0 - 100 °C
176 - 212 °F
Drying Temperature 90.0 - 100 °C

@Time 10800 sec
194 - 212 °F

@Time 3.00 hour
Descriptive Properties Value Comments
ISO Shrinkage - Pressure 60 MPa