Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.240 J/cm² | 1.14 ft-lb/in² | ISO 180 |
Nanocyl PLASTICYL™ PP2001 Polypropylene with 5 wt% Multi-Wall Carbon Nanotubes PLASTICYL™ is a family of Multi-Wall Carbon Nanotube (MWNT) thermoplastic concentrates for applications requiring superior electrical conductivity and electrostatic discharge (ESD) properties. PLA.. |
|||
Charpy Impact, Notched | 0.240 - 4.10 J/cm² | 1.14 - 19.5 ft-lb/in² | Average value: 0.912 J/cm² Grade Count:29 |
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar.. |
|||
Charpy Impact, Notched | 0.240 J/cm² @Temperature -30.0 °C |
1.14 ft-lb/in² @Temperature -22.0 °F |
|
Ineos ABS Centrex® 485 ASA+AES Blend
(discontinued **) Key Features:UnfilledLight stabilized or stable to lightU.V. stabilized or stable to weatherSuitable processing methods:Profile extrusionSheet extrusionThermoformingInformation provided by Bayer Pol.. |
|||
Charpy Impact, Notched | 0.240 J/cm² @Temperature -20.0 °C |
1.14 ft-lb/in² @Temperature -4.00 °F |
DIN 53453 |
Global PP-2340-TC Polypropylene Block Copolymer Description-opacity, medium to high stiffness, high impact strength at low temperatureApplications-electrical appliances, bases, panels, auto parts, cupsInformation provided by Global Polymers Corp.. |
|||
Charpy Impact, Notched | 0.240 J/cm² @Temperature 23.0 °C |
1.14 ft-lb/in² @Temperature 73.4 °F |
DIN 53453 |
IRPC Polimaxx Polene 1100RC Polypropylene Homopolymer CHARACTERISTICS: HIGH FLOW, GOOD STIFFNESS, GOOD PROCESSABILITY, GOOD MELT STABILITYAPPLICATIONS: INJECTION MOLDING FOR THIN WALL PARTS, HOUSE WARES EXTRUSION COATING FOR COATED WOVEN BAGS AND TARPA.. |
|||
Charpy Impact, Notched | 0.240 J/cm² @Temperature 23.0 °C |
1.14 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Grupo Repol Dinalon® B1S25 PA6 Unreinforced Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol |
|||
Charpy Impact, Notched | 0.239 J/cm² | 1.14 ft-lb/in² | ASTM D256 |
Plenco 00757 Melamine-Phenolic, Granular, Transfer Molded PLENCO 00757 is a melamine-phenolic, copolymer molding compound, offering excellent arc resistance and comparative track index values. It is formulated to provide improved mechanical strength proper.. |
|||
Charpy Impact, Notched | 0.240 J/cm² | 1.14 ft-lb/in² | ISO 179 |
Unitika TERRAMAC TE-7300 Polylactic Acid (PLA) Heat-resisting grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Charpy Impact, Notched | 0.240 J/cm² @Temperature 23.0 °C |
1.14 ft-lb/in² @Temperature 73.4 °F |
EN ISO 179 |
Ensinger TECASINT™ 2021 Polyimide, Brown (PI) TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications... |
|||
Charpy Impact, Notched | 0.240 J/cm² | 1.14 ft-lb/in² | ISO 179 1eA |
Azoty Tarnow™ Tarnamid® T-27 GF20 FRV2 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grade, flammability class V2, reinforced with 20% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning... |
|||
Charpy Impact, Notched | 0.240 - 0.320 J/cm² | 1.14 - 1.52 ft-lb/in² | Average value: 0.290 J/cm² Grade Count:4 |
Overview of materials for Polypropylene, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Carbon Fiber 10%". Each property range of values reported is minimum and maximum values o.. |