Material Notes:
PLENCO 00757 is a melamine-phenolic, copolymer molding compound, offering excellent arc resistance and comparative track index values. It is formulated to provide improved mechanical strength properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 00757 is available only in brown.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.610 g/cc
0.0220 lb/in³
ASTM D1895
Density 1.71 g/cc
0.0618 lb/in³
ASTM D792
Water Absorption 0.28 %
0.28 %
ASTM D570
Linear Mold Shrinkage 0.0049 cm/cm
0.0049 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 73
73
ASTM D785
Tensile Strength, Ultimate 53.0 MPa
7690 psi
ASTM D638
Elongation at Break 0.47 %
0.47 %
ASTM D638
Tensile Modulus 12.7 GPa
1840 ksi
ASTM D638
Flexural Strength 90.0 MPa
13100 psi
ASTM D790
Flexural Modulus 11.1 GPa
1610 ksi
ASTM D790
Compressive Strength 155 MPa
22500 psi
ASTM D695
Izod Impact, Notched 0.215 J/cm
0.403 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.239 J/cm²
1.14 ft-lb/in²
ASTM D256
Impact 125
125
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 165 °C
329 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 187 °C
369 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.00 mm
V-0

@Thickness 0.0394 in
Shrinkage 0.36 %
0.36 %
240 hr, 105ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 1.30e+12 ohm-cm
1.30e+12 ohm-cm
ASTM D247
Dielectric Constant 6.8
6.8
ASTM D150
Dielectric Strength 6.80 kV/mm
173 kV/in
Step by Step; ASTM D149
9.50 kV/mm
241 kV/in
Short Time; ASTM D149
Dissipation Factor 0.069
0.069
ASTM D150
Arc Resistance 188 sec
188 sec
ASTM D495
Comparative Tracking Index 600 V
600 V
ASTM D3638