Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.240 - 0.320 J/cm²
1.14 - 1.52 ft-lb/in²
Average value: 0.290 J/cm² Grade Count:4
Overview of materials for Polypropylene, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Carbon Fiber 10%". Each property range of values reported is minimum and maximum values o..