Polymer Property : Charpy Impact, Notched = 0.240 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.240 J/cm²
1.14 ft-lb/in²
ISO 180
Nanocyl PLASTICYL™ PP2001 Polypropylene with 5 wt% Multi-Wall Carbon Nanotubes
PLASTICYL™ is a family of Multi-Wall Carbon Nanotube (MWNT) thermoplastic concentrates for applications requiring superior electrical conductivity and electrostatic discharge (ESD) properties. PLA..
Charpy Impact, Notched 0.240 - 4.10 J/cm²
1.14 - 19.5 ft-lb/in²
Average value: 0.912 J/cm² Grade Count:29
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar..
Charpy Impact, Notched 0.240 J/cm²

@Temperature -30.0 °C
1.14 ft-lb/in²

@Temperature -22.0 °F
Ineos ABS Centrex® 485 ASA+AES Blend  (discontinued **)
Key Features:UnfilledLight stabilized or stable to lightU.V. stabilized or stable to weatherSuitable processing methods:Profile extrusionSheet extrusionThermoformingInformation provided by Bayer Pol..
Charpy Impact, Notched 0.240 J/cm²

@Temperature -20.0 °C
1.14 ft-lb/in²

@Temperature -4.00 °F
DIN 53453
Global PP-2340-TC Polypropylene Block Copolymer
Description-opacity, medium to high stiffness, high impact strength at low temperatureApplications-electrical appliances, bases, panels, auto parts, cupsInformation provided by Global Polymers Corp..
Charpy Impact, Notched 0.240 J/cm²

@Temperature 23.0 °C
1.14 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
IRPC Polimaxx Polene 1100RC Polypropylene Homopolymer
CHARACTERISTICS: HIGH FLOW, GOOD STIFFNESS, GOOD PROCESSABILITY, GOOD MELT STABILITYAPPLICATIONS: INJECTION MOLDING FOR THIN WALL PARTS, HOUSE WARES EXTRUSION COATING FOR COATED WOVEN BAGS AND TARPA..
Charpy Impact, Notched 0.240 J/cm²

@Temperature 23.0 °C
1.14 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Grupo Repol Dinalon® B1S25 PA6 Unreinforced
Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol
Charpy Impact, Notched 0.240 J/cm²
1.14 ft-lb/in²
ISO 179
Unitika TERRAMAC TE-7300 Polylactic Acid (PLA)
Heat-resisting grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd.
Charpy Impact, Notched 0.240 J/cm²

@Temperature 23.0 °C
1.14 ft-lb/in²

@Temperature 73.4 °F
EN ISO 179
Ensinger TECASINT™ 2021 Polyimide, Brown (PI)
TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications...
Charpy Impact, Notched 0.240 J/cm²
1.14 ft-lb/in²
ISO 179 1eA
Azoty Tarnow™ Tarnamid® T-27 GF20 FRV2 Polyamide 6 - Flame Retarded, Reinforced
Flame retarded grade, flammability class V2, reinforced with 20% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning...
Charpy Impact, Notched 0.240 - 0.320 J/cm²
1.14 - 1.52 ft-lb/in²
Average value: 0.290 J/cm² Grade Count:4
Overview of materials for Polypropylene, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Carbon Fiber 10%". Each property range of values reported is minimum and maximum values o..