EMS-Grivory Grivory® BRZ 340 H PA6

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® BRZ 340 H PA6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product description: Grilon BRZ 340 H is a heat stabilized, high viscosity, impact modified PA6 extrusion grade. Grilon BRZ 340 H has the following important properties:High impact strength at low temperatures High flexibilityLow density Grilon BRZ 340 H is used typically for automotive applications which demand high flexibility and toughness such as flexible tubes and fuel tubes.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
ISO 1183
Water Absorption 9.0 %
9.0 %
ISO 62
Moisture Absorption 3.00 %
3.00 %
ISO 62
Mechanical Properties Metric English Comments
Ball Indentation Hardness 45.0 MPa
6530 psi
conditioned; ISO 2039-1
130 MPa
18900 psi
dry; ISO 2039-1
Tensile Strength at Break 40.0 MPa
5800 psi
dry; ISO 527-1/-2
45.0 MPa
6530 psi
conditioned; ISO 527-1/-2
Tensile Strength, Yield 35.0 MPa
5080 psi
dry; ISO 527-1/-2
70.0 MPa
10200 psi
dry; ISO 527-1/-2
Elongation at Break 40 %
40 %
dry; ISO 527-1/-2
40 %
40 %
dry; ISO 527-1/-2
>= 50 %
>= 50 %
conditioned; ISO 527-1/-2
Elongation at Yield 4.0 %
4.0 %
dry; ISO 527-1/-2
15 %
15 %
conditioned; ISO 527-1/-2
Tensile Modulus 0.700 GPa
102 ksi
conditioned; ISO 527-1/-2
2.80 GPa
406 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched NB
NB
dry; ISO 179/1eU
NB
NB
conditioned; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
dry; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 1.50 J/cm²
7.14 ft-lb/in²
dry; ISO 179/1eA
NB
NB
conditioned; ISO 179/1eA
0.700 J/cm²

@Temperature 30.0 °C
3.33 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
1.10 J/cm²

@Temperature 30.0 °C
5.23 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 90.0 µm/m-°C
50.0 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 120 µm/m-°C
66.7 µin/in-°F
ISO 11359-1/-2
Melting Point 222 °C
432 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 100 - 120 °C
212 - 248 °F
long term; EMS
180 °C
356 °F
short term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 130 °C
266 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
conditioned; IEC 60093
1.00e+14 ohm-cm
1.00e+14 ohm-cm
dry; IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Strength 35.0 kV/mm
889 kV/in
conditioned; IEC 60243-1
40.0 kV/mm
1020 kV/in
dry; IEC 60243-1
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Air intake sytems
Cooling and climate control
Electricals & Electronics Cables & Tubes
Form Granules
Industry & Consumer goods Hydraulics & Pneumatics
Mechanical Engineering
Power transmission
Processing Other Extrusion