Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Murtfeldt Muralen® Black Antistatic Polyethylene, Conductive

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), UHMW PE Ultra High Molecular Weight
Manufacturer Murtfeldt Kunststoffe GmbH & Co
Trade Name Muralen®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Murtfeldt Muralen® Black Antistatic Polyethylene, Conductive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Muralen® is based on high molecular weight polyethylene (PE-HMW) and is ideally suited for use in applications that require the generally impressive material properties of polyethylene. Because of its great cut, impact, and shock resistance, this material is often used to make underlays for cutting and punching machines and for ram guards.Special Properties:• High cut resistance• Good shock and impact absorption• Good resistance to chemicals• Good anti-adhesion properties• Approved for use in the food industry (EU and FDA) • Good weldability• AntistaticInformation provided by Murtfeldt Kunststoffe GmbH & Co. KG.
Physical Properties Metric English Comments
Density <= 0.950 g/cc
<= 0.0343 lb/in³
ISO 1183
Molecular Weight 500000 g/mol
500000 g/mol
Mechanical Properties Metric English Comments
Hardness, Shore D 66
66
DIN 53505
Ball Indentation Hardness 45.0 MPa
6530 psi
Tensile Strength 25.0 MPa
3630 psi
ISO 527
Elongation at Break 580 %
580 %
ISO 527
Modulus of Elasticity 1.10 GPa
160 ksi
Charpy Impact, Notched >= 2.50 J/cm²
>= 11.9 ft-lb/in²
ISO 179
Coefficient of Friction, Dynamic 0.18
0.18
Sand Slurry 350
350
value in %
Thermal Properties Metric English Comments
CTE, linear 200 µm/m-°C

@Temperature 23.0 - 60.0 °C
111 µin/in-°F

@Temperature 73.4 - 140 °F
Thermal Conductivity 0.400 W/m-K
2.78 BTU-in/hr-ft²-°F
ISO 52612
Maximum Service Temperature, Air 80.0 °C

@Time 1.80e+7 sec
176 °F

@Time 5000 hour
Minimum Service Temperature, Air -100 °C
-148 °F
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.00e+6 ohm-cm
>= 1.00e+6 ohm-cm
IEC 60093
Surface Resistance >= 1.00e+9 ohm
>= 1.00e+9 ohm
IEC 60093
Compliance Properties Metric English Comments
FDA Yes
Yes
Descriptive Properties Value Comments
Color Black