Material Notes:
Product description: Grilon TSS is an unreinforced, heat stabilized, normal viscosity PA66 + PA6 injection molding grade. Grilon TSS has the following important properties: Excellent flow behaviorHigh toughnessVery good surface finishEasy processing Grilon TSS is used typically for various applications in the automotive-, the electro and the sports & leisure field such as loudspeaker grids, interior casings, chair rollers, handles and levers.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183
Water Absorption 9.0 %
9.0 %
ISO 62
Moisture Absorption 3.00 %
3.00 %
ISO 62
Linear Mold Shrinkage, Flow 0.011 cm/cm
0.011 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.013 cm/cm
0.013 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Ball Indentation Hardness 45.0 MPa
6530 psi
conditioned; ISO 2039-1
135 MPa
19600 psi
dry; ISO 2039-1
Tensile Strength at Break 45.0 MPa
6530 psi
dry; ISO 527-1/-2
Tensile Strength, Yield 40.0 MPa
5800 psi
dry; ISO 527-1/-2
70.0 MPa
10200 psi
dry; ISO 527-1/-2
Elongation at Break 25 %
25 %
dry; ISO 527-1/-2
25 %
25 %
dry; ISO 527-1/-2
>= 50 %
>= 50 %
conditioned; ISO 527-1/-2
Elongation at Yield 4.0 %
4.0 %
dry; ISO 527-1/-2
15 %
15 %
conditioned; ISO 527-1/-2
Tensile Modulus 0.750 GPa
109 ksi
conditioned; ISO 527-1/-2
2.70 GPa
392 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched NB
NB
dry; ISO 179/1eU
NB
NB
conditioned; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
dry; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
dry; ISO 179/1eA
3.50 J/cm²
16.7 ft-lb/in²
conditioned; ISO 179/1eA
0.600 J/cm²

@Temperature 30.0 °C
2.86 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
0.700 J/cm²

@Temperature 30.0 °C
3.33 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 80.0 µm/m-°C
44.4 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 120 µm/m-°C
66.7 µin/in-°F
ISO 11359-1/-2
Melting Point 260 °C
500 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 80.0 - 110 °C
176 - 230 °F
long term; EMS
180 °C
356 °F
short term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
conditioned; IEC 60093
1.00e+13 ohm-cm
1.00e+13 ohm-cm
dry; IEC 60093
Surface Resistance 1.00e+10 ohm
1.00e+10 ohm
IEC 60093
Dielectric Strength 25.0 kV/mm
635 kV/in
conditioned; IEC 60243-1
26.0 kV/mm
660 kV/in
dry; IEC 60243-1
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Automotive electr. and electronics, lighting
Interior
Electricals & Electronics Connectors
Electrical appliances
Form Granules
Industry & Consumer goods Mechanical Engineering
Power transmission
Sports & Leisure
Tools & Accessories
Processing Injection Molding
Product Attributes Nucleated
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved