Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 160 - 170 MPa | 23200 - 24700 psi | Average value: 163 MPa Grade Count:3 |
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% .. |
|||
Ball Indentation Hardness | 130 - 170 MPa | 18900 - 24700 psi | Average value: 147 MPa Grade Count:7 |
Overview of materials for Phenolic, Novolac, Fabric Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Fabric Filled". Each property range of values reported is minimum and maximum values .. |
|||
Ball Indentation Hardness | 90.0 - 170 MPa | 13100 - 24700 psi | Average value: 121 MPa Grade Count:7 |
Overview of materials for Nylon 66/6 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6". Each property range of values reported is minimum and maximum values of appropriate MatWeb .. |
|||
Ball Indentation Hardness | 100 - 170 MPa @Time 30.0 sec |
14500 - 24700 psi @Time 0.00833 hour |
DIN 53 456 |
Hippe PA 66 Nylon 66 The polyamide with high degree of hardness, stiffness, scuff strength and stability of shape under heat. Preferred polyamide for components subjected to high load and heat stress in electrical, mec.. |
|||
Ball Indentation Hardness | 160 - 170 MPa | 23200 - 24700 psi | Average value: 167 MPa Grade Count:6 |
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m.. |
|||
Ball Indentation Hardness | 165 - 170 MPa | 23900 - 24700 psi | Average value: 168 MPa Grade Count:4 |
Overview of materials for Polyetherimide (PEI) This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate Mat.. |