Material Notes:
Product description: Grilamid XE 3915 is a 50% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following produce profile:Good UV StabilityHigh impact strengthVery dimensionally stableVery low shrinkage Grilamid XE 3915 is suitable for production of technical parts in the application fields of: ElectroElectronicsAutomotiveSafety technologyMechanical engineeringDomestic appliancesInformation provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.47 g/cc
0.0531 lb/in³
ISO 1183
Water Absorption 0.80 %
0.80 %
ISO 62
Moisture Absorption 0.400 %
0.400 %
ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cm
0.0010 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0050 cm/cm
0.0050 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Hardness, Shore D 82
82
conditioned, 15s; ISO 868
Ball Indentation Hardness 155 MPa
22500 psi
conditioned; ISO 2039-1
Tensile Strength at Break 135 MPa
19600 psi
conditioned; ISO 527-1/-2
155 MPa
22500 psi
dry; ISO 527-1/-2
Elongation at Break 6.0 %
6.0 %
dry; ISO 527-1/-2
6.0 %
6.0 %
conditioned; ISO 527-1/-2
Tensile Modulus 11.5 GPa
1670 ksi
conditioned; ISO 527-1/-2
13.0 GPa
1890 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 8.00 J/cm²
38.1 ft-lb/in²
conditioned; ISO 179/1eU
8.50 J/cm²
40.4 ft-lb/in²
dry; ISO 179/1eU
8.00 J/cm²

@Temperature 30.0 °C
38.1 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
8.50 J/cm²

@Temperature 30.0 °C
40.4 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
Charpy Impact, Notched 2.00 J/cm²
9.52 ft-lb/in²
conditioned; ISO 179/1eA
2.10 J/cm²
9.99 ft-lb/in²
dry; ISO 179/1eA
1.50 J/cm²

@Temperature 30.0 °C
7.14 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
1.60 J/cm²

@Temperature 30.0 °C
7.61 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 15.0 µm/m-°C
8.33 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 120 µm/m-°C
66.7 µin/in-°F
ISO 11359-1/-2
Melting Point 178 °C
352 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 90.0 - 120 °C
194 - 248 °F
long term; EMS
150 °C
302 °F
short term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 165 °C
329 °F
ISO 75-1/-2
Deflection Temperature at 8.0 MPa 125 °C
257 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
conditioned; IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Strength 35.0 kV/mm
889 kV/in
conditioned; IEC 60243-1
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Automotive electr. and electronics, lighting
Compressed air systems
Exterior
Hydraulic systems
Electricals & Electronics Connectors
Electrical appliances
Electrical equipment
Mobile phones and other portable devices
Form Granules
Industry & Consumer goods Housewares
Mechanical Engineering
Medical devices
Power transmission
Sports & Leisure
Tools & Accessories
Processing Injection Molding
Special Characteristics High impact or impact modified
Improved heat resistance
Improved UV resistance (outdoor use)
Users viewing this material also viewed the following: