Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 0.339 J @Thickness 3.17 mm |
0.250 ft-lb @Thickness 0.125 in |
Falling Weight; ASTM D-3029 GB |
Plaskolite Optix® CP - 51 KC General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Gardner Impact | 0.339 J @Thickness 3.17 mm |
0.250 ft-lb @Thickness 0.125 in |
Falling Weight; ASTM D-3029 GB |
Plaskolite Optix® CP - 61 General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Gardner Impact | 0.339 J @Thickness 3.17 mm |
0.250 ft-lb @Thickness 0.125 in |
Falling Weight; ASTM D-3029 GB |
Plaskolite West Optix® CP - 51 KC General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Gardner Impact | 0.339 J @Thickness 3.17 mm |
0.250 ft-lb @Thickness 0.125 in |
Falling Weight; ASTM D-3029 GB |
Plaskolite West Optix® CP - 61 General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Gardner Impact | 0.339 J | 0.250 ft-lb | ASTM D5420 |
RheTech Products F15-01 35% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black Applications: HousingsBattery traysInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.339 J | 0.250 ft-lb | ASTM D5420 |
RheTech Products F22-01 20% Glass Fiber/Mineral Co-Reinforced Polypropylene, Black Applications: Support ductsHousingsBattery traysInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.339 J | 0.250 ft-lb | ASTM D5420 |
RheTech Products F55-01 43% Glass Fiber/Talc Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Consumer goodsSupportsGolf cart bracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.339 J | 0.250 ft-lb | ASTM D5420 |
RheTech Products FRG130-01 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Flame Retardant, Black Applications: Electrical component housingsSunroof componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.339 J | 0.250 ft-lb | ASTM D5420 |
RheTech Products G10P100-00 10% Glass Fiber Reinforced Polypropylene, Natural Applications: BracketsIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.339 J | 0.250 ft-lb | ASTM D5420 |
RheTech Products G10UP100-01 10% Glass Fiber Reinforced Polypropylene, Black, UL94-HB Rated Applications: Consumer housingsConsumer goodsFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.339 J | 0.250 ft-lb | ASTM D5420 |
RheTech Products G13P100-00 13% Glass Fiber Reinforced Polypropylene, Natural Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.339 J | 0.250 ft-lb | ASTM D5420 |
RheTech Products G13P100-332UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, (GM 9772) Light Neutral Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.339 J | 0.250 ft-lb | ASTM D5420 |
RheTech Products G13P100-347UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, 109D Medium Pewter Applications: Dome lamp housingsFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.339 J | 0.250 ft-lb | ASTM D5420 |
RheTech Products G13P100-553UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, (GM 501F) Dark Smoke Gray Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.339 J | 0.250 ft-lb | ASTM D5420 |
RheTech Products G13P100-559UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, (GM WPP 646H) Charcoal Metallic Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.339 J | 0.250 ft-lb | ASTM D5420 |
RheTech Products G13P100-598UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, (NH-293L) Seagull Gray Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.339 J | 0.250 ft-lb | ASTM D5420 |
RheTech Products G13P100-724UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, NH220L Clear Gray Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.339 J | 0.250 ft-lb | ASTM D5420 |
RheTech Products GC10P100-00 10% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural Applications: Air ducts - distributionFuel filler pocketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.339 J | 0.250 ft-lb | ASTM D5420 |
RheTech Products GC30P101-00 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural Applications: BracketsHead lamp housingsBattery trayFan shroudInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.339 J | 0.250 ft-lb | ASTM D5420 |
RheTech Products GC30P103-01 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black Applications: Battery traysFender apronsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.339 J | 0.250 ft-lb | ASTM D5420 |
RheTech Products GC30P104-01 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black Applications: BracketsHead lamp housingsBattery trayInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.339 J | 0.250 ft-lb | ASTM D5420 |
RheTech Products GC43P250-00 43% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural Applications: Consumer goodsFunctional supportsHead lamp bracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.339 J | 0.250 ft-lb | ASTM D5420 |
RheTech Products F15-00UV 35% Glass Fiber Reinforced Polypropylene, Chemically Coupled, UV-Stabilized, Natural Applications: Functional SupportsElectrical housingsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.339 J | 0.250 ft-lb | ASTM D5420 |
RheTech Products M15P101-01 15% Mica Reinforced Polypropylene, Black Applications: Air ducts - distributionFan shroudsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.339 J | 0.250 ft-lb | per mil; ASTM D-4226 |
Axiall HHP-190 Rigid PVC, Extrusion Georgia Gulf HHP-190 is a special purpose profile extrusion alloy designed for applications requiring the following properties: Heat Resistance & Thermal StabilityImpact Strength & ToughnessDimensi.. |
|||
Gardner Impact | 0.339 J | 0.250 ft-lb | per mil; ASTM D-4226 |
Axiall HHW-191 Rigid PVC, Extrusion Georgia Gulf HHW-191 is a special purpose profile extrusion alloy designed for applications requiring the following properties: Excellent WeatherabilityImpact Strength & ToughnessColorabilityChemic.. |
|||
Gardner Impact | 0.339 J | 0.250 ft-lb | ASTM D5420 |
RheTech Products GC30P104-00 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural Applications: BracketsHead lamp housingsBattery trayInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.339 J | 0.250 ft-lb | ASTM D5420 |
RheTech Products GC43P250-01 43% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Consumer goodsFunctional supportsHead lamp bracketsDurable GoodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.339 - 4.52 J | 0.250 - 3.33 ft-lb | Average value: 0.693 J Grade Count:22 |
Overview of materials for Polypropylene, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum .. |
|||
Gardner Impact | 0.339 - 4.07 J | 0.250 - 3.00 ft-lb | Average value: 2.82 J Grade Count:3 |
Overview of materials for Polypropylene with 10% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Mica Filler". Specific grades with primary filler content between 5% and 14% are .. |