Mechanical Properties Metric English Comments
Gardner Impact 0.339 - 4.07 J
0.250 - 3.00 ft-lb
Average value: 2.82 J Grade Count:3
Overview of materials for Polypropylene with 10% Mica Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Mica Filler". Specific grades with primary filler content between 5% and 14% are ..