Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Axiall HHW-191 Rigid PVC, Extrusion

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall HHW-191 Rigid PVC, Extrusion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Georgia Gulf HHW-191 is a special purpose profile extrusion alloy designed for applications requiring the following properties: Excellent WeatherabilityImpact Strength & ToughnessColorabilityChemical ResistanceHeat Resistance and Thermal StabilityDimensional Stability in Dark ColorsFlame Retardant Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.24 g/cc
1.24 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110
110
ASTM D-785
Hardness, Shore D 80
80
ASTM D-2240
Tensile Strength, Yield 46.2 MPa
6700 psi
ASTM D-638
Tensile Modulus 2.41 GPa
350 ksi
ASTM D-638
Flexural Strength 75.8 MPa
11000 psi
ASTM D-790
Flexural Modulus 2.41 GPa
350 ksi
ASTM D-790
Izod Impact, Notched 5.34 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
10.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D-256
Gardner Impact 0.339 J
0.250 ft-lb
per mil; ASTM D-4226
Tensile Impact Strength 94.5 kJ/m²
45.0 ft-lb/in²
ASTM D-1822
Thermal Properties Metric English Comments
CTE, linear 73.8 µm/m-°C

@Temperature 20.0 °C
41.0 µin/in-°F

@Temperature 68.0 °F
ASTM D-696
Deflection Temperature at 1.8 MPa (264 psi) 88.3 °C
191 °F
ASTM D-648
Flammability, UL94 V-1
V-1
At 0.125 inch
Processing Properties Metric English Comments
Zone 1 149 °C
300 °F
Zone 2 154 °C
310 °F
Zone 3 160 °C
320 °F
Zone 4 166 °C
330 °F
Zone 5 171 °C
340 °F
Die Temperature 177 °C
350 °F
Melt Temperature 188 - 199 °C
370 - 390 °F
Copyright © lookpolymers.com All Rights Reserved